Fast screening of Sulfide Stress Corrosion resistance of Supermartensitic Stainless Steel thought alternative test methods

In order to meet growing energy demand, oil and gas industries are facing many challenges, including the exploitation of increasingly deep fields with high pressure and high temperature in sour environments containing CO2 and H2S. Operators must carefully select materials that are resistant to these aggressive environments. The main risk associated with the use of martensitic stainless steels is the risk of sulfide stress cracking under well shut-in conditions.
The aim of this study is to evaluate the performance of supermartensitic stainless steels (13Cr-5Ni- 2Mo) based on NACE TM-0177-2016 method A and alternative methods such as slow strain rate test according to TM-0198-2016 and ripple strain rate test. Cyclic potentiodynamic polarization measurements were also performed to evaluate pitting and repassivation performance. The interest of this study is to present reliable and fast criteria to predict sulfide stress cracking performance of supermartensitic stainless steels through alternative methods. The effect of buffer and chloride content on pitting resistance and sulfide stress corrosion cracking resistance will also be discussed as well as the effect of Mo and Cr on pitting resistance.

Product Number: 51320-14577-SG
Author: Martien Duvall, Cécile Millet, Daniela Garcia, Guilaume Neel, Harold Evin
Publication Date: 2020