98495 Effect of Composition and Corrosion Properties of the Metallic Matrix on the Erosion-Corrosion Behavior of HVOF Sprayed WC-Coatings

Product Number: 51300-98495-SG
ISBN: 98495 1998 CP
Author: Trond Rogne, Tone Solem, John Berget
$0.00
$20.00
$20.00
In corrosive media the wear resistance of ceramic-metallic coatings is dependent on the corrosion resistance of the metal matrix. Other factors that will affect the coating deterioration are the corrosivity of the medium and any galvanic interaction from the surrounding material. This paper presents results from a study where different types of WC(Co/Cr/Mo/Ni) powders have been sprayed by HVOF, Diamond Jet 2600 Hybrid equipment. The properties of the sprayed coatings have been verified by metallographic studies and by erosion-corrosion testing both under corrosive and non-corrosive conditions. The results clearly demonstrate the importance of having a metal matrix at least as corrosion resistance as the surrounding materials. When wear exposed components in pipe systems, pumps or valves are coated with a WC type coating, the corrosion resistance of the metal matrix should be compatible to the material of the rest of the system. This is especially important when the surrounding materials are corrosion resistant alloys as stainless steels, where the coatings otherwise will act as an anode. Keywords: Ceramic-metallic coatings, Metal phase, HVOF, Composition, Corrosion, Erosion
In corrosive media the wear resistance of ceramic-metallic coatings is dependent on the corrosion resistance of the metal matrix. Other factors that will affect the coating deterioration are the corrosivity of the medium and any galvanic interaction from the surrounding material. This paper presents results from a study where different types of WC(Co/Cr/Mo/Ni) powders have been sprayed by HVOF, Diamond Jet 2600 Hybrid equipment. The properties of the sprayed coatings have been verified by metallographic studies and by erosion-corrosion testing both under corrosive and non-corrosive conditions. The results clearly demonstrate the importance of having a metal matrix at least as corrosion resistance as the surrounding materials. When wear exposed components in pipe systems, pumps or valves are coated with a WC type coating, the corrosion resistance of the metal matrix should be compatible to the material of the rest of the system. This is especially important when the surrounding materials are corrosion resistant alloys as stainless steels, where the coatings otherwise will act as an anode. Keywords: Ceramic-metallic coatings, Metal phase, HVOF, Composition, Corrosion, Erosion
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for 99048 Corrosion, Erosion-Corrosion and Wear
Available for download

99048 Corrosion, Erosion-Corrosion and Wear Resistance of HVOF Sprayed WC Type Coatings with a Corrosion Resistant Binder

Product Number: 51300-99048-SG
ISBN: 99048 1999 CP
Author: Tone Solem, Trend Rogne and John Berget
$20.00
Picture for 99295 EROSION/CORROSION OF HVOF SPRAYED
Available for download

99295 EROSION/CORROSION OF HVOF SPRAYED COATINGS.

Product Number: 51300-99295-SG
ISBN: 99295 1999 CP
Author: S. Simard, B. Arsenault, J.G. Legoux, H. M. Hawthorne
$20.00
Picture for 98482 “The Effect of Surface Iron Contamination
Available for download

98482 “The Effect of Surface Iron Contamination on the Corrosion Resistance of Alloys in Simulated FGD Environments”

Product Number: 51300-98482-SG
ISBN: 98482 1998 CP
Author: William L Silence, Paul Crook, Jeffrey R. Dillman, F.G. Hodge
$20.00