99295 EROSION/CORROSION OF HVOF SPRAYED COATINGS.

Product Number: 51300-99295-SG
ISBN: 99295 1999 CP
Author: S. Simard, B. Arsenault, J.G. Legoux, H. M. Hawthorne
$0.00
$20.00
$20.00
Cermet based materials are known to have an excellent performance under several different wear conditions. High velocity oxy-fuel (HVOF) thermal spraying technology allows the deposition of such hard materials in the form of protective coatings onto different surfaces. Under slurry erosion, the performance of the coating is influenced by the occurrence of corrosion reactions with the metallic matrix. Slurry erosion tests were conducted with a jet impingement rig with a 9.1 wt% alumina particle/water slurry. Indeed, wet conditions promote the dissolution of metallic binder resulting in a potential synergy between the corrosion and wear mechanisms. Coatings based on tungsten carbide embedded in four different metallic binders were evaluated with regard to wear and corrosion. Depending on the composition of the metallic binder, different degradation rates were observed.
Cermet based materials are known to have an excellent performance under several different wear conditions. High velocity oxy-fuel (HVOF) thermal spraying technology allows the deposition of such hard materials in the form of protective coatings onto different surfaces. Under slurry erosion, the performance of the coating is influenced by the occurrence of corrosion reactions with the metallic matrix. Slurry erosion tests were conducted with a jet impingement rig with a 9.1 wt% alumina particle/water slurry. Indeed, wet conditions promote the dissolution of metallic binder resulting in a potential synergy between the corrosion and wear mechanisms. Coatings based on tungsten carbide embedded in four different metallic binders were evaluated with regard to wear and corrosion. Depending on the composition of the metallic binder, different degradation rates were observed.
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for Erosion-Corrosion Study of Oilfield Materials Due to Liquid Impact
Available for download
Picture for 08572 Erosion-Corrosion in Disturbed Liquid/Particle Flow
Available for download

08572 Erosion-Corrosion in Disturbed Liquid/Particle Flow

Product Number: 51300-08572-SG
ISBN: 08572 2008 CP
Author: Joshua Addis, Srdjan Nesic, and Bruce Brown
Publication Date: 2008
$20.00
Picture for 01513 HIGH TEMPERATURE EROSION RESISTANT
Available for download

01513 HIGH TEMPERATURE EROSION RESISTANT MATERIALS FOR PETROLEUM REFINERY EQUIPMENT

Product Number: 51300-01513-SG
ISBN: 01513 2001 CP
Author: Damodaran Raghu, Brad McKee, Cliff Sheriff, and James B. C. Wu
$20.00