Amine units are generally used in refineries and petrochemical plants to remove acid gases such as hydrogen sulfide (H2S) and carbon dioxide (C02) from process streams. Commonly, corrosion of carbon steels in amine units is not caused by the amine itself but by its reaction with dissolved gases. In this paper, fundamental aspects concerning the susceptibility of carbon steels to stress corrosion cracking in amine solutions are presented, and special attention is given to a recent study on a commercial mixture of amines. An overview is made on the methodology used.
Amine units are generally used in refineries and petrochemical plants to remove acid gases such as hydrogen sulfide (H2S) and carbon dioxide (C02) from process streams. Commonly, corrosion of carbon steels in amine units is not caused by the amine itself but by its reaction with dissolved gases. In this paper, fundamental aspects concerning the susceptibility of carbon steels to stress corrosion cracking in amine solutions are presented, and special attention is given to a recent study on a commercial mixture of amines. An overview is made on the methodology used.
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for 96394 CORROSIVE AMINE CHARACTERIZATION
Available for download

96394 CORROSIVE AMINE CHARACTERIZATION

Product Number: 51300-96394-SG
ISBN: 96394 1996 CP
Author: H. Lee Craig Jr., B. D. McLaughlin
$20.00
Picture for 09334 Failure of Amine Regenerating Column of Amine Treatment Unit
Available for download

09334 Failure of Amine Regenerating Column of Amine Treatment Unit

Product Number: 51300-09334-SG
ISBN: 09334 2009 CP
Author: Nitin D. Raut, V. S. Naik and R. M. Chaudhari
Publication Date: 2009
$20.00
Picture for 00492 CAUSES OF AMINE PLANT CORROSION- DESIGN
Available for download

00492 CAUSES OF AMINE PLANT CORROSION- DESIGN CONSIDERATIONS

Product Number: 51300-00492-SG
ISBN: 00492 2000 CP
Author: Sidney F Bosen, Ph.D.
$20.00