If unprotected, seawater lift pump caissons can suffer severe galvanic corrosion. Within 2-5 years holes in the caisson can appear. The corrosion to the steel caissons is caused by the noble pumps and risers, which normally are made of Ni-Al-bronze, and/or (super) duplex stainless steel. If the caisson is not protected by a coating, corrosion rates of 2-5 mm/year are reported. For coated caissons, corrosion rates of more than 10 mm/year have been seen. This extreme high rate is caused by galvanic current concentration in small coating defects.

This article will describe how corrosion was stopped on coated caissons on a FPSO. Also installation of a cathodic protection system for relatively smaller pumps on two platforms in the Northsea will be discussed. Intensive reference cell measurements confirmed that the position of the sacrificial anodes is crucial. For this reason an effective way of hanging the anodes in the annulus of the pump and riser in the caisson was developed. Duplex and super duplex stainless steels should not be protected at levels more electronegative than - 900 mV Ag/AgCl. This is achieved by a potential control unit on the sacrificial anode assemblies.
If unprotected, seawater lift pump caissons can suffer severe galvanic corrosion. Within 2-5 years holes in the caisson can appear. The corrosion to the steel caissons is caused by the noble pumps and risers, which normally are made of Ni-Al-bronze, and/or (super) duplex stainless steel. If the caisson is not protected by a coating, corrosion rates of 2-5 mm/year are reported. For coated caissons, corrosion rates of more than 10 mm/year have been seen. This extreme high rate is caused by galvanic current concentration in small coating defects.

This article will describe how corrosion was stopped on coated caissons on a FPSO. Also installation of a cathodic protection system for relatively smaller pumps on two platforms in the Northsea will be discussed. Intensive reference cell measurements confirmed that the position of the sacrificial anodes is crucial. For this reason an effective way of hanging the anodes in the annulus of the pump and riser in the caisson was developed. Duplex and super duplex stainless steels should not be protected at levels more electronegative than - 900 mV Ag/AgCl. This is achieved by a potential control unit on the sacrificial anode assemblies.
Product tags
Also Purchased
Picture for 06105 Corrosion problems in seawater pump
Available for download

06105 Corrosion problems in seawater pump caissons. Practical solutions.

Product Number: 51300-06105-SG
ISBN: 06105 2006 CP
Author: Svenn Magne Wigen, Harald Osvoll
$20.00
Picture for Experience with Standard Duplex Stainless Steel Seawater Pump in Arabian Gulf Seawater Conditions
Available for download

51314-3733-Experience with Standard Duplex Stainless Steel Seawater Pump in Arabian Gulf Seawater Conditions

Product Number: 51314-3733-SG
ISBN: 3733 2014 CP
Author: Sivuyile Funani
Publication Date: 2014
$0.00