Studies were carried out to evaluate the stress corrosion cracking (SCC) behavior of a X-70 microalloyed pipeline steel, with different microstructures by means of the slow strain rate testing (SSRT) technique at 50 ºC. Tests solutions consisted of 0.1, 0.05, 0.01 and 0.005 M sodium bicarbonate (NaHCO3) with KCl, CaCl2 and MgSO4-7H2O additions. Different anodic and cathodic potentials were applied. Additionally, experiments using the SSRT technique but with pre-charged hydrogen samples and potentiodynamic curves at different sweep rates were also done to elucidate hydrogen effects in this type of steel. The results showed that the different microstructures in conjunction with the anodic applied potentials shift the cracking susceptibility of the steels evaluated.
Studies were carried out to evaluate the stress corrosion cracking (SCC) behavior of a X-70 microalloyed pipeline steel, with different microstructures by means of the slow strain rate testing (SSRT) technique at 50 ºC. Tests solutions consisted of 0.1, 0.05, 0.01 and 0.005 M sodium bicarbonate (NaHCO3) with KCl, CaCl2 and MgSO4-7H2O additions. Different anodic and cathodic potentials were applied. Additionally, experiments using the SSRT technique but with pre-charged hydrogen samples and potentiodynamic curves at different sweep rates were also done to elucidate hydrogen effects in this type of steel. The results showed that the different microstructures in conjunction with the anodic applied potentials shift the cracking susceptibility of the steels evaluated.
Product tags
Also Purchased
Picture for 03447 STRESS CORROSION CRACKING BEHAVIOR OF
Available for download

03447 STRESS CORROSION CRACKING BEHAVIOR OF MICROALLOYED PIPELINE STEELS EXPOSED TO PRESSURIZED SOUR GAS ENVIRONMENTS

Product Number: 51300-03447-SG
ISBN: 03447 2003 CP
Author: J. L. Albarran, O. Flores, G. Gonzalez, R. Perez
$20.00
Picture for 06175 Stress Corrosion Cracking of Pipeline Steel
Available for download

06175 Stress Corrosion Cracking of Pipeline Steel in Near-Neutral pH Environments

Product Number: 51300-06175-SG
ISBN: 06175 2006 CP
Author: Stefanie L. Asher, Jeffery A. Colwell, Preet M. Singh, Brian N. Leis
$20.00