UNS S32101 is a general-purpose lean duplex stainless steel with low nickel content. The stress corrosion cracking properties of UNS S32101 were investigated under constant strain conditions. Both evaporative and immersion test methods were used. The results for UNS S32101 were compared with those of a standard austenitic stainless steel and other duplex grades. Immersed in concentrated chloride solutions, UNS S32101 exhibited similar resistance to stress corrosion cracking as other duplex grades. In the wick test UNS S32101 was not susceptible to stress corrosion cracking and was comparable to other duplex grades while the austenitic grade tested failed due to stress corrosion cracking. When exposed to chloride deposits under atmospheric conditions UNS S32101along with other duplex grades, did not suffer from stress corrosion cracking while the austenitic grade did. Thus, the chloride stress corrosion cracking resistance of UNS S32101 was shown to be far superior to that of austenitic grade UNS S30400. Moreover, UNS S32101 displays behaviour similar to other duplex steel grades tested. With the test methods used, it was not possible to obtain an individual ranking of the different duplex stainless steel grades.
UNS S32101 is a general-purpose lean duplex stainless steel with low nickel content. The stress corrosion cracking properties of UNS S32101 were investigated under constant strain conditions. Both evaporative and immersion test methods were used. The results for UNS S32101 were compared with those of a standard austenitic stainless steel and other duplex grades. Immersed in concentrated chloride solutions, UNS S32101 exhibited similar resistance to stress corrosion cracking as other duplex grades. In the wick test UNS S32101 was not susceptible to stress corrosion cracking and was comparable to other duplex grades while the austenitic grade tested failed due to stress corrosion cracking. When exposed to chloride deposits under atmospheric conditions UNS S32101along with other duplex grades, did not suffer from stress corrosion cracking while the austenitic grade did. Thus, the chloride stress corrosion cracking resistance of UNS S32101 was shown to be far superior to that of austenitic grade UNS S30400. Moreover, UNS S32101 displays behaviour similar to other duplex steel grades tested. With the test methods used, it was not possible to obtain an individual ranking of the different duplex stainless steel grades.
Product tags
Also Purchased
Picture for 10342 Properties of a New Lean Duplex Alloy
Available for download

10342 Properties of a New Lean Duplex Alloy

Product Number: 51300-10342-SG
ISBN: 10342 2010 CP
Author: John F. Grubb, Bahri Ozturk, David S. Bergstrom, and John J. Dunn
Publication Date: 2010
$20.00
Picture for 07474 Stress Corrosion Cracking of Duplex Stainless Steels under Simulated Evaporation Conditions
Available for download

07474 Stress Corrosion Cracking of Duplex Stainless Steels under Simulated Evaporation Conditions

Product Number: 51300-07474-SG
ISBN: 07474 2007 CP
Author: Alan Turnbull, Gareth Hinds, Shengqi Zhou, and Patrick Nicholson
Publication Date: 2007
$20.00