The susceptibility of 22 Cr and 25 Cr duplex stainless steels to stress corrosion cracking under evaporative seawater conditions has been evaluated using a modified drop evaporation test. Failure of both steels occurred at temperatures as low as 105 °C. Observation of patchy corrosion and occasional pitting beneath the salt layer suggests that the underdeposit chemistry was aggressive for this system and a combination of this chemistry and micro-plastic deformation is considered to be responsible for cracking of the steels. The engineering implication is that existing recommendations for the critical temperature for coating of duplex stainless steel to avoid failures in service may need to be revised.
The susceptibility of 22 Cr and 25 Cr duplex stainless steels to stress corrosion cracking under evaporative seawater conditions has been evaluated using a modified drop evaporation test. Failure of both steels occurred at temperatures as low as 105 °C. Observation of patchy corrosion and occasional pitting beneath the salt layer suggests that the underdeposit chemistry was aggressive for this system and a combination of this chemistry and micro-plastic deformation is considered to be responsible for cracking of the steels. The engineering implication is that existing recommendations for the critical temperature for coating of duplex stainless steel to avoid failures in service may need to be revised.
Product tags
Also Purchased
Picture for 11255 Pitting Corrosion Mechanisms of Lean Duplex
Available for download

11255 Pitting Corrosion Mechanisms of Lean Duplex, Duplex and Super Duplex Stainless Steels in Chloride Solutions

Product Number: 51300-11255-SG
ISBN: 2011 11255 CP
Author: J. Saithala, J. Atkinson, H Ubhi, A. Patil
Publication Date: 2011
$20.00
Picture for 07476 Assessment of Methods to Prevent Chloride SCC Propagation in Stainless Steels
Available for download

07476 Assessment of Methods to Prevent Chloride SCC Propagation in Stainless Steels

Product Number: 51300-07476-SG
ISBN: 07476 2007 CP
Author: Thierry Cassagne, Patrice Castagna, Claude Duret, and Tong Eak Pou
Publication Date: 2007
$20.00
Picture for 07475 Stress Corrosion Cracking Properties of UNS S32101 - A New Duplex Stainless Steel with Low Nic
Available for download

07475 Stress Corrosion Cracking Properties of UNS S32101 - A New Duplex Stainless Steel with Low Nickel Content

Product Number: 51300-07475-SG
ISBN: 07475 2007 CP
Author: Elisabeth Johansson and Tomas Prosek
Publication Date: 2007
$20.00