03510 STRESS CORROSION CRACKING SUSCEPTIBILITY OF ALUMINUM-SILICON-BRONZE

Product Number: 51300-03510-SG
ISBN: 03510 2003 CP
Author: J.J. Hoffman, J.W. Slusser, J.L. O’Leary
$0.00
$20.00
$20.00
A laboratory program was initiated to study the stress corrosion cracking susceptibility of aluminum-silicon-bronze (copper alloy C64210) valves used in gaseous fluorine (F2) service. Some testing was also performed with 303 SS (UNS S30300) valves. The threaded outlet connections of the valves were torqued to different values and wetted with 3 wt% hydrofluoric acid (HF) (to simulate a small F2 leak), 5% potassium iodide (KI), or commercial leak detection solution. Branched, intergranular cracks initiated in all the test environments at the highly stressed thread root areas indicating that crack initiation was primarily dependent on the torque applied to the outlet connection. The aluminum-siliconbronze material also experienced dealloying corrosion upon exposure to the hydrofluoric acid and potassium iodide solutions. The compatibility of the alloys in fluorine service is discussed. Keywords: aluminum-silicon-bronze, UNS C64210, UNS S30300, stress corrosion cracking, fluorine, hydrofluoric acid, potassium iodine, dealloying
A laboratory program was initiated to study the stress corrosion cracking susceptibility of aluminum-silicon-bronze (copper alloy C64210) valves used in gaseous fluorine (F2) service. Some testing was also performed with 303 SS (UNS S30300) valves. The threaded outlet connections of the valves were torqued to different values and wetted with 3 wt% hydrofluoric acid (HF) (to simulate a small F2 leak), 5% potassium iodide (KI), or commercial leak detection solution. Branched, intergranular cracks initiated in all the test environments at the highly stressed thread root areas indicating that crack initiation was primarily dependent on the torque applied to the outlet connection. The aluminum-siliconbronze material also experienced dealloying corrosion upon exposure to the hydrofluoric acid and potassium iodide solutions. The compatibility of the alloys in fluorine service is discussed. Keywords: aluminum-silicon-bronze, UNS C64210, UNS S30300, stress corrosion cracking, fluorine, hydrofluoric acid, potassium iodine, dealloying
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for 03262 EFFECT OF COMPOSITION AND MICROSTRUCTURE
Available for download

03262 EFFECT OF COMPOSITION AND MICROSTRUCTURE ON THE SEAWATER CORROSION RESISTANCE OF NICKEL-ALUMINUM BRONZE

Product Number: 51300-03262-SG
ISBN: 03262 2003 CP
Author: Harold T. Michels, Robert M. Kain
$20.00
Picture for 04294 Corrosion Assessment of Nickel Aluminum
Available for download

04294 Corrosion Assessment of Nickel Aluminum Bronze (NAB) in Seawater

Product Number: 51300-04294-SG
ISBN: 04294 2004 CP
Author: Kunigahalli L. Vasanth and Richard A. Hays, Naval Surface Warfare Center
$20.00
Picture for 04301 The Environmental Factors Affecting the
Available for download

04301The Environmental Factors Affecting the Performance of Nickel Aluminum Bronze

Product Number: 51300-04301-SG
ISBN: 04301 2004 CP
Author: Rakesh C. Barik, J.A. Wharton, and Robert J.K. Wood, University of Southampton; K.R. Stokes, Winfrit
$20.00