The stress corrosion crack growth rate of alloy 182 weld metal and alloy 600 was studied under highly controlled water chemistry conditions at 288 °C. This continuing program has focused on the strong effects of corrosion potential, water purity, dissolved H2... KeyWords: alloy 600, alloy 182, weld metal, stress corrosion cracking, high temperature water, crack growth rate corrosion potential, water purity, stress intensity factor, cold work, sensitization.
The stress corrosion crack growth rate of alloy 182 weld metal and alloy 600 was studied under highly controlled water chemistry conditions at 288 °C. This continuing program has focused on the strong effects of corrosion potential, water purity, dissolved H2... KeyWords: alloy 600, alloy 182, weld metal, stress corrosion cracking, high temperature water, crack growth rate corrosion potential, water purity, stress intensity factor, cold work, sensitization.
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for 00222 STRESS CORROSION CRACK GROWTH IN ALLOY
Available for download

00222 STRESS CORROSION CRACK GROWTH IN ALLOY 600 EXPOSED TO PWR AND BWR ENVIRONMENTS

Product Number: 51300-00222-SG
ISBN: 00222 2000 CP
Author: Markus O. Speidel and Ruth Magdowski
$20.00
Picture for 02495 Comparison and Ranking of Techniques for...
Available for download

02495 Comparison and Ranking of Techniques for Monitoring General and Pitting Corrosion Rates Inside Pipelines

Product Number: 51300-02495-SG
ISBN: 02495 2002 CP
Author: Sankara Papavinasam, R.Winston Revie, Alebachew Demoz, and Kirk Michaelian
$20.00
Picture for 02493 EROSION CORROSION PHENOMENA OF...
Available for download

02493 EROSION CORROSION PHENOMENA OF 13Cr ALLOY IN FLOWS CONTAINING SAND PARTICLES

Product Number: 51300-02493-SG
ISBN: 02493 2002 CP
Author: H. Rincon, J. Chen, and J. Shadley
$20.00