51313-02086-Resistance to Stress Corrosion Cracking of Duplex Stainless Steels

Product Number: 51313-02086-SG
ISBN: 02086 2013 CP
Author: Sandra Le Manchet
Publication Date: 2013
$0.00
$20.00
$20.00
Corrosion resistant alloys are widely used in many industrial processes. They include a wide range of materials from 13%Cr martensitic stainless steels up to nickel-based alloys. Among them duplex materials have aroused great interest for various applications: pulp&paper thermal desalination and oil&gas industries.This paper reviews stress corrosion cracking data related to some duplex stainless steel grades in chloride-containing media. Experimental data obtained from various techniques (slow strain rate constant load U-bend and four point bending) are reported. The objective is to point out the influence of some key parameters such as temperature and chloride content on the resistance of these grades.Key words: Duplex stainless steel chloride stress corrosion cracking
Corrosion resistant alloys are widely used in many industrial processes. They include a wide range of materials from 13%Cr martensitic stainless steels up to nickel-based alloys. Among them duplex materials have aroused great interest for various applications: pulp&paper thermal desalination and oil&gas industries.This paper reviews stress corrosion cracking data related to some duplex stainless steel grades in chloride-containing media. Experimental data obtained from various techniques (slow strain rate constant load U-bend and four point bending) are reported. The objective is to point out the influence of some key parameters such as temperature and chloride content on the resistance of these grades.Key words: Duplex stainless steel chloride stress corrosion cracking
Product tags
Also Purchased
Picture for Duplex Stainless Steel Chloride Stress Corrosion Cracking Risk in Refining
Available for download

51313-02520-Duplex Stainless Steel Chloride Stress Corrosion Cracking Risk in Refining

Product Number: 51313-02520-SG
ISBN: 02520 2013 CP
Author: Karly Moore
Publication Date: 2013
$20.00
Picture for 09300 Stress Corrosion Cracking of Super Duplex Stainless Steels above and below Pitting Potentials
Available for download

09300 Stress Corrosion Cracking of Super Duplex Stainless Steels above and below Pitting Potentials

Product Number: 51300-09300-SG
ISBN: 09300 2009 CP
Author: Janardhan Rao Saithala, John Atkinson, Harvindher Singh Ubhi, Andy Houghton and Steve McCoy
Publication Date: 2009
$20.00
Picture for 11255 Pitting Corrosion Mechanisms of Lean Duplex
Available for download

11255 Pitting Corrosion Mechanisms of Lean Duplex, Duplex and Super Duplex Stainless Steels in Chloride Solutions

Product Number: 51300-11255-SG
ISBN: 2011 11255 CP
Author: J. Saithala, J. Atkinson, H Ubhi, A. Patil
Publication Date: 2011
$20.00