Recent Advances in Hybrid Laser-Arc Welding of Thick Steel Plates

With the objective of reducing the number of welding passes in thick plate welding, hybrid laser-arc welding technique was utilized to one-pass weld 25mm thick steel plates. Butt joints were designed with a square groove and 2.5mm air gap. Either ceramic strip or submerged arc welding flux was used for joint backing. The joint gap was filled up with cut-wire particles of the same chemical compositions as those of the arc welding filler wire. Cut-wire particles were inserted to protect the backing material from direct interaction with the laser irradiation. Welding parameters were optimized to obtain full penetration joints without damaging the backing material. Square groove butt joints of 25mm thickness were successfully welded in one welding pass. Similarly, 50 mm thick square groove butt joints could be double-side welded

Product Number: MPWT19-15295
Author: Mohamed Wahba, Masami Mizutani, Seiji Katayama
Publication Date: 2019
$0.00
$0.00
$0.00
Product tags
Also Purchased
Picture for Effects of Welding on Flow Accelerated Corrosion of Carbon Steel Pipes
Available for download

51314-4301-Effects of Welding on Flow Accelerated Corrosion of Carbon Steel Pipes

Product Number: 51314-4301-SG
ISBN: 4301 2014 CP
Author: Seifollah Nasrazadani
Publication Date: 2014
$0.00
Picture for Sulfide Stress Corrosion Cracking of a Spiral Weld Pipeline in Sour Service
Available for download

51314-3835-Sulfide Stress Corrosion Cracking of a Spiral Weld Pipeline in Sour Service

Product Number: 51314-3835-SG
ISBN: 3835 2014 CP
Author: Abdul Razzaq Al-Shamari
Publication Date: 2014
$0.00