Influence of Shear Stress on the Pitting Corrosion Susceptibility of Austenitic Stainless Steel in Brine Evaluated in the Rotating Cylinder Electrode

During drilling operations the drillstring might be subjected to downhole conditions leading to pitting corrosion. State-of-the-art directional drilling technologies are very demanding in terms of material requirements including corrosion resistance. Manganese-stabilized fully austenitic stainless steels in strain-hardened condition own a beneficial combination of high strength high ductility and high toughness by keeping their own non-magnetic character. Therefore CrMn-stainless steels have been extensively used in drilling equipment. Once in contact with high chloride bearing drilling fluids at elevated temperatures however their passivity is compromised leading to pit nucleation and propagation. In consequence the pitting corrosion resistance of these materials becomes a significant limiting factor for their selection as well as for assessing the service life of drillstring components. To date extensive research work has been conducted to characterize the pitting susceptibility of CrMn-stainless steels under static conditions. Little attention however has been paid to the effect of shear stresses introduced by the flow of the drilling fluid on the pitting resistance and damage morphology produced on these materials when exposed to brines at elevated temperatures. To address this electrochemical examinations were conducted using the rotating cylinder electrode (RCE). The present paper discusses the results from potentiodynamic polarization tests and their relation to the hydrodynamic conditions produced in the RCE at different temperatures.

Product Number: 51319-13362-SG
Author: Helmuth Sarmiento Klapper
Publication Date: 2019
$0.00
$20.00
$20.00
Also Purchased
Picture for Effect of Wall Shear Stress on Sour Corrosion of Carbon Steel
Available for download

51314-4051-Effect of Wall Shear Stress on Sour Corrosion of Carbon Steel

Product Number: 51314-4051-SG
ISBN: 4051 2014 CP
Author: Chong Li
Publication Date: 2014
$20.00
Picture for 01069 Does Shear Stress Have an Effect on
Available for download

01069 Does Shear Stress Have an Effect on Corrosion in Sour Gas Production?

Product Number: 51300-01069-SG
ISBN: 01069 2001 CP
Author: Buddy Short, James A. Dougherty, Sunder Ramachandran
$20.00
Picture for 02199 ELECTROCHEMICAL INVESTIGATION OF HIGH...
Available for download

02199 ELECTROCHEMICAL INVESTIGATION OF HIGH VELOCITY OXY-FUEL (HVOF) ALUMINUM BRONZE COATINGS UNDER SLURRY EROSION IN SALINE ENVIRONMENTS

Product Number: 51300-02199-SG
ISBN: 02199 2002 CP
Author: KS Tan, RJK Wood, JA Wharton, and KR Stokes
$20.00