51316-7901-Fatigue Behavior under Multiaxial Loading and Simulated Geothermal Environment of Cr-Mn-N Austenitic Steel and UNS N07718

Product Number: 51316-7901-SG
ISBN: 7901 2016 CP
Author: Helmuth Sarmiento Klapper
Publication Date: 2016
$0.00
$20.00
$20.00
~~The fatigue life and reliability of components for modern drilling technologies are restricted by severe environmental conditions. The mechanical strain caused by drilling through hard formations in combination with increasing temperatures due to large drilling depths typical for depth geothermal wells and in corrosive media are particular critical for metallic materials. Therefore for testing materials a suitable test rig which enables to mimic the simultaneous influence of multiaxial fatigue loading elevated temperatures and corrosive environments is necessary. Because of the complexity of this type of testing the use of non-contacting 3D measurement techniques and thermography was considered. Also a special specimen geometry was developed. The influence of surface quality temperature loading conditions and corrosion on the fatigue life and reliability of one Cr-Mn-N austenitic steel and alloy 718 has been evaluated. These materials are commonly used in drilling applications due to their high strength high ductility non-magnetic behavior and good corrosion resistance. The failure mechanisms were studied in detail by means of scanning electron microscopy and x-ray diffraction.
~~The fatigue life and reliability of components for modern drilling technologies are restricted by severe environmental conditions. The mechanical strain caused by drilling through hard formations in combination with increasing temperatures due to large drilling depths typical for depth geothermal wells and in corrosive media are particular critical for metallic materials. Therefore for testing materials a suitable test rig which enables to mimic the simultaneous influence of multiaxial fatigue loading elevated temperatures and corrosive environments is necessary. Because of the complexity of this type of testing the use of non-contacting 3D measurement techniques and thermography was considered. Also a special specimen geometry was developed. The influence of surface quality temperature loading conditions and corrosion on the fatigue life and reliability of one Cr-Mn-N austenitic steel and alloy 718 has been evaluated. These materials are commonly used in drilling applications due to their high strength high ductility non-magnetic behavior and good corrosion resistance. The failure mechanisms were studied in detail by means of scanning electron microscopy and x-ray diffraction.
Product tags
Also Purchased
Picture for Establishing Operating Envelops for Material Susceptibility to Environmentally Assisted Cracking in
Available for download

51316-7892-Establishing Operating Envelops for Material Susceptibility to Environmentally Assisted Cracking in Thermal Oil Sands Operation

Product Number: 51316-7892-SG
ISBN: 7892 2016 CP
Author: Tesfaalem Gebremedhin Haile
Publication Date: 2016
$20.00
Picture for Qualification of Integral Dinned UNS S32205 Heat Exchanger Tubing for Refinery Wet H2S se
Available for download

51316-7887-Qualification of Integral Dinned UNS S32205 Heat Exchanger Tubing for Refinery Wet H2S se

Product Number: 51316-7887-SG
ISBN: 7887 2016 CP
Author: Ivan Morales
Publication Date: 2016
$20.00
Picture for Modeling and Prediction of Corrosion of Steel Tubular in SAGD/CO2 Co-Injection System
Available for download

51316-7888-Modeling and Prediction of Corrosion of Steel Tubular in SAGD/CO2 Co-Injection System

Product Number: 51316-7888-SG
ISBN: 7888 2016 CP
Author: Frank Cheng
Publication Date: 2016
$20.00