Search
Filters
Close

51316-7592-Effect of ppb Levels of Chloride on the Stress Corrosion Cracking of Pressure Vessel Steel

Product Number: 51316-7592-SG
ISBN: 7592 2016 CP
Author: Xiaoyuan Lou
Publication Date: 2016
$0.00
$20.00
$20.00
This talk covers the results from a 4-year program of evaluating the effect of very low levels of chloride (< 5ppb) on the stress corrosion cracking (SCC) behavior of low-alloy pressure vessel steel (A533B) in high temperature water. Three different heats of low alloy steel from reactor vessels were evaluated under both periodical partial unloading condition and constant load/K condition. Effects of chloride (1-5 ppb) stress intensity factor (K) specimen orientation and hydrogen chemistry were studied in detail. It was found that the compositional percentage of sulfur is a weak measure of SCC susceptibility under ppb level of chloride. The potential reason that may cause heat-to-heat difference on SCC suscetibility will also be discussed. The result from this program suggests that the chloride level as low as 2-4 ppb can increase the SCC susceptibility of low alloy steel in BWR environment.
This talk covers the results from a 4-year program of evaluating the effect of very low levels of chloride (< 5ppb) on the stress corrosion cracking (SCC) behavior of low-alloy pressure vessel steel (A533B) in high temperature water. Three different heats of low alloy steel from reactor vessels were evaluated under both periodical partial unloading condition and constant load/K condition. Effects of chloride (1-5 ppb) stress intensity factor (K) specimen orientation and hydrogen chemistry were studied in detail. It was found that the compositional percentage of sulfur is a weak measure of SCC susceptibility under ppb level of chloride. The potential reason that may cause heat-to-heat difference on SCC suscetibility will also be discussed. The result from this program suggests that the chloride level as low as 2-4 ppb can increase the SCC susceptibility of low alloy steel in BWR environment.
Product tags
Also Purchased
Picture for 10287 Critical Stress Corrosion Cracking Potentials of Stainless Steels in Dilute Chloride Solutions
Available for download

10287 Critical Stress Corrosion Cracking Potentials of Stainless Steels in Dilute Chloride Solutions

Product Number: 51300-10287-SG
ISBN: 10287 2010 CP
Author: Janardhan Rao Saithala, Steve McCoy, John Atkinson and Harvindher Singh Ubhi
Publication Date: 2010
$20.00