51312-01723-Characterization of Age-Hardenable Superalloy for Advanced Ultrasupercritical Service

Product Number: 51312-01723-SG
ISBN: 01723 2012 CP
Author: Brian A. Baker
Publication Date: 2012
$0.00
$20.00
$20.00
Results from characterization of commercial large-section piping and superheater tubing will be presented. The response of alloy 740H to oxidation and coal-ash corrosion testing within the framework of expected benchmarks for advanced ultra supercritical boiler service will be discussed. In addition mechanical and physical properties of the commercial product will be presented.
Results from characterization of commercial large-section piping and superheater tubing will be presented. The response of alloy 740H to oxidation and coal-ash corrosion testing within the framework of expected benchmarks for advanced ultra supercritical boiler service will be discussed. In addition mechanical and physical properties of the commercial product will be presented.
Product tags
Also Purchased
Picture for Morphologies of MIC in Copper and Carbon Steel Tubes - Case Histories
Available for download

51312-01711-Morphologies of MIC in Copper and Carbon Steel Tubes - Case Histories

Product Number: 51312-01711-SG
ISBN: 01711 2012 CP
Author: Ewa M. Labuda
Publication Date: 2012
$20.00
Picture for Improvement of the Oxidation Behavior of Ferritic-Martensitic Steels in Water Vapor Containing Envir
Available for download

51312-01725-Improvement of the Oxidation Behavior of Ferritic-Martensitic Steels in Water Vapor Containing Envir

Product Number: 51312-01725-SG
ISBN: 01725 2012 CP
Author: Diana Schmidt
Publication Date: 2012
$20.00
Picture for Materials Selection for Designing SAGD Plants
Available for download

51312-01716-Materials Selection for Designing SAGD Plants

Product Number: 51312-01716-SG
ISBN: 01716 2012 CP
Author: Dilip Kumar
Publication Date: 2012
$20.00