99324 PITTING CORROSION ON WELD JOINTS OFFSHORE STRUCTURE JACKETS

Product Number: 51300-99324-SG
ISBN: 99324 1999 CP
Author: P.F. ANTO
$0.00
$20.00
$20.00
During underwater inspection, pitting corrosion was observed on various weld joints of offshore structure jackets. For this purpose, during underwater inspection surveys cathodic protection potentials were measured at different locations on the jackets. The position and condition of anodes were also examined. Pitting and galvanic corrosion studies and cathodic protection experiments were carried out in synthetic sea water and in 3.5% NaCl solution. Field exposure studies were also carried out. The present paper describes the investigations carried out to determine reasons for pitting corrosion on weld joints and remedial measures. Key words : pitting corrosion, weld joints, offshore structure jacket, cathodic protection
During underwater inspection, pitting corrosion was observed on various weld joints of offshore structure jackets. For this purpose, during underwater inspection surveys cathodic protection potentials were measured at different locations on the jackets. The position and condition of anodes were also examined. Pitting and galvanic corrosion studies and cathodic protection experiments were carried out in synthetic sea water and in 3.5% NaCl solution. Field exposure studies were also carried out. The present paper describes the investigations carried out to determine reasons for pitting corrosion on weld joints and remedial measures. Key words : pitting corrosion, weld joints, offshore structure jacket, cathodic protection
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for 05277 Preferential Weld Corrosion: Effects of
Available for download

05277 Preferential Weld Corrosion: Effects of Weldment Microstructure and Composition

Product Number: 51300-05277-SG
ISBN: 05277 2005 CP
Author: Chi-Ming Lee and Paul Woollin, TWI Ltd.
$20.00
Picture for 97447 UNDER-DEPOSIT CORROSION AT WELD
Available for download

97447 UNDER-DEPOSIT CORROSION AT WELD SEAMS IN CARBON STEEL PIPING

Product Number: 51300-97447-SG
ISBN: 97447 1997 CP
Author: Andrew G. Howell
$20.00
Picture for 99277 CORROSION EVALUATION OF STAINLESS STEEL
Available for download

99277 CORROSION EVALUATION OF STAINLESS STEEL ROOT WELD SHIELDING

Product Number: 51300-99277-SG
ISBN: 99277 1999 CP
Author: Margaret Gorog and Linda Sawyer
$20.00