99171 MIC ON STAINLESS STEELS IN WASTEWATER TREATMENT PLANTS

Product Number: 51300-99171-SG
ISBN: 99171 1999 CP
Author: A. Iversen
$0.00
$20.00
$20.00
Field tests of stainless steels were carried out at five wastewater treatment plants for one year. Three stainless steel grades i.e. AISI 304 (UNS S30400), AISI 316 (UNS S31600) and duplex 2205 (UNS S31803)were tested in the final settling tank in the plants. The time dependence of the open circuit potential (OCP) was measured for all coupons. Ennoblement of the OCP, similar to that reported from investigations in seawater, was found in one of the plants. Waters from three of the exposure sites, containing dispersed deposits from exposed coupons, were chemically analyzed. Pitting corrosion was observed after the field test on steel grade AISI 304 in three of the five plants, and on AISI 316 in one plant. No corrosion was found on 2205 in any of the plants. Laboratory measurements of the OCP were carried out for AISI 304, AISI 316 and 2205 in water collected from one of the plants. Cathodic polarization curves were determined as well in wastewater fi-om the same plant. The cathodic reaction rate increased at the highest OCP. Simulation of the ennoblement was carried out by potentiostatic polarization in a 600 ppm chloride solution. The current response indicated corrosion on AISI 304 welded material and on AISI 304, AISI 316 in crevice assemblies after a long period of induction time, Keywords: MIC, Wastewater, Stainless steels, Potential ennoblement, Cathodic reaction
Field tests of stainless steels were carried out at five wastewater treatment plants for one year. Three stainless steel grades i.e. AISI 304 (UNS S30400), AISI 316 (UNS S31600) and duplex 2205 (UNS S31803)were tested in the final settling tank in the plants. The time dependence of the open circuit potential (OCP) was measured for all coupons. Ennoblement of the OCP, similar to that reported from investigations in seawater, was found in one of the plants. Waters from three of the exposure sites, containing dispersed deposits from exposed coupons, were chemically analyzed. Pitting corrosion was observed after the field test on steel grade AISI 304 in three of the five plants, and on AISI 316 in one plant. No corrosion was found on 2205 in any of the plants. Laboratory measurements of the OCP were carried out for AISI 304, AISI 316 and 2205 in water collected from one of the plants. Cathodic polarization curves were determined as well in wastewater fi-om the same plant. The cathodic reaction rate increased at the highest OCP. Simulation of the ennoblement was carried out by potentiostatic polarization in a 600 ppm chloride solution. The current response indicated corrosion on AISI 304 welded material and on AISI 304, AISI 316 in crevice assemblies after a long period of induction time, Keywords: MIC, Wastewater, Stainless steels, Potential ennoblement, Cathodic reaction
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for 02451 MIC ON STAINLESS STEELS IN WASTEWATER...
Available for download

02451 MIC ON STAINLESS STEELS IN WASTEWATER TREATMENT PLANTS FIELD TESTS AND A RISK ASSESSMENT

Product Number: 51300-02451-SG
ISBN: 02451 2002 CP
Author: A. Iversen
$20.00
Picture for 03563  MIC OF STAINLESS STEEL PIPES IN SEWAGE
Available for download

03563 MIC OF STAINLESS STEEL PIPES IN SEWAGE TREATMENT PLANTS

Product Number: 51300-03563-SG
ISBN: 03563 2003 CP
Author: T. Mathiesen, E. Rislund, T.S. Nielsen, J.E. Frantsen
$20.00
Picture for 03562 MIC ON STAINLESS STEELS IN WASTEWATER
Available for download