98319 EVALUATION OF PITTING CORROSION WITH ELECTROCHEMICAL IMPEDANCE SPECTROSCOPY (EIS) FOR ALUMINA/ALUMINUM ALLOY COMPOSITES

Product Number: 51300-98319-SG
ISBN: 98319 1998 CP
Author: Charles Odegard, Arturo Bronson
$0.00
$20.00
$20.00
The pitting susceptibility of monolithic aluminum 6061 alloy and alumina/aluminum alloy composites has been analyzed by using electrochemical impedance spectroscopy and subsequent comparison with their polarization scans. The composites consisting of 0.10 and 0.15 volume fraction of alumina particles (VFAP) and the monolith as cylindrical electrodes were rotated at 1500 rpm while immersed in NaCl solution. The passive currents of the composites were greater than that of the monolith as per the polarization scans. The impedance spectra were acquired at constant potential increments along the passive region up to the pitting potential. The impedance spectra represented by semicircles on a Nyquist plot acquired above the pitting potential collapsed underneath the spectra obtained in the passive region near the corrosion potential for the monolithic alloy and composites. The impedance spectra modeled with a simplified equivalent circuit indicate that the effective capacitance for the composites is greater than that of the monolithic alloy. Keywords: pitting, localized corrosion, impedance spectroscopy, capacitance
The pitting susceptibility of monolithic aluminum 6061 alloy and alumina/aluminum alloy composites has been analyzed by using electrochemical impedance spectroscopy and subsequent comparison with their polarization scans. The composites consisting of 0.10 and 0.15 volume fraction of alumina particles (VFAP) and the monolith as cylindrical electrodes were rotated at 1500 rpm while immersed in NaCl solution. The passive currents of the composites were greater than that of the monolith as per the polarization scans. The impedance spectra were acquired at constant potential increments along the passive region up to the pitting potential. The impedance spectra represented by semicircles on a Nyquist plot acquired above the pitting potential collapsed underneath the spectra obtained in the passive region near the corrosion potential for the monolithic alloy and composites. The impedance spectra modeled with a simplified equivalent circuit indicate that the effective capacitance for the composites is greater than that of the monolithic alloy. Keywords: pitting, localized corrosion, impedance spectroscopy, capacitance
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for 98302 A TUTORIAL ON IMPEDANCE SPECTROSCOPY
Available for download

98302 A TUTORIAL ON IMPEDANCE SPECTROSCOPY

Product Number: 51300-98302-SG
ISBN: 98302 1998 CP
Author: Mark E. Orazem
$20.00
Picture for 98305 APPLICATIONS OF LPR TO THIN FILM LIQUID
Available for download

98305 APPLICATIONS OF LPR TO THIN FILM LIQUID PHASES

Product Number: 51300-98305-SG
ISBN: 98305 1998 CP
Author: K. M. Lawson,M. Yunovich, D. L. Caudill
$20.00
Picture for 98301 Applications and Problem Solving Using
Available for download

98301 Applications and Problem Solving Using the Polarization Technique

Product Number: 51300-98301-SG
ISBN: 98301 1998 CP
Author: Ann Chidester Van Orden
$20.00