Server maintenance is scheduled for Saturday, December 21st between 6am-10am CST.

During that time, parts of our website will be affected until maintenance is completed. Thank you for your patience.

Search
Filters
Close

98261 STRESS CORROSION BEHAVIOR OF Ru-ENHANCED ALPHA-BETA TITANIUM ALLOYS IN METHANOL SOLUTIONS

Product Number: 51300-98261-SG
ISBN: 98261 1998 CP
Author: T.A. Bednarowicz, R.W. Schutz, J.M. Horrigan
$0.00
$20.00
$20.00
Conservative, practical guidelines for the minimum water content required to prevent methanolic stress corrosion cracking (SCC) of Ti-6Al-4V-Ru and Ti-3AI-2.5V-Ru alloy tubulars have been developed from slow strain rate testing in plain and acidified NaCl-saturated methanol-water solutions at 25°C. A minimum methanol water content of 10 wt.% is proposed for Ti-6Al-4V-Ru, whereas 2-3 wt.% is sufficient for the lower strength Ti-3Al-2.5V-Ru alloy. Although HCl-acidification aggravated methanolic SCC, intermixing of methanol with crude oil or pure hydrocarbons, H2S gas saturation, and/or increasing temperature diminished cracking susceptibility in these ahoy tubulars. Keywords: titanium alloys, ruthenium, methanol, crude oil, pipe, stress corrosion cracking, inhibition
Conservative, practical guidelines for the minimum water content required to prevent methanolic stress corrosion cracking (SCC) of Ti-6Al-4V-Ru and Ti-3AI-2.5V-Ru alloy tubulars have been developed from slow strain rate testing in plain and acidified NaCl-saturated methanol-water solutions at 25°C. A minimum methanol water content of 10 wt.% is proposed for Ti-6Al-4V-Ru, whereas 2-3 wt.% is sufficient for the lower strength Ti-3Al-2.5V-Ru alloy. Although HCl-acidification aggravated methanolic SCC, intermixing of methanol with crude oil or pure hydrocarbons, H2S gas saturation, and/or increasing temperature diminished cracking susceptibility in these ahoy tubulars. Keywords: titanium alloys, ruthenium, methanol, crude oil, pipe, stress corrosion cracking, inhibition
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for 97493 Materials Experience in Methanol Reforming
Available for download

97493 Materials Experience in Methanol Reforming Units

Product Number: 51300-97493-SG
ISBN: 97493 1997 CP
Author: K. L. Baumert, J. J. Hoffman
$20.00
Picture for Methanol-Induced Internal Stress Corrosion Cracking in a Northern Petroleum Pipeline
Available for download

51314-3985-Methanol-Induced Internal Stress Corrosion Cracking in a Northern Petroleum Pipeline

Product Number: 51314-3985-SG
ISBN: 3985 2014 CP
Author: Barbara Padgett
Publication Date: 2014
$20.00
Picture for 03536 STRESS CORROSION CRACKING OF H.C.P.
Available for download

03536 STRESS CORROSION CRACKING OF H.C.P. METALS AND ALLOYS IN IODINE-METHANOL SOLUTIONS

Product Number: 51300-03536-SG
ISBN: 03536 2003 CP
Author: S. B. Farina, G. S. Duffo, J. R. Galvele
$20.00