98156 GALVANIC CORROSION STUDY OF CONTAINER MATERIALS USING ZERO RESISTANCE AMMETER

Product Number: 51300-98156-SG
ISBN: 98156 1998 CP
Author: Ajit K. Roy, Demiis L. Fleming, Beverly Y. Lum
$0.00
$20.00
$20.00
Galvanic corrosion behavior of A 5 16 steel separately coupled to six different corrosion-resistant alloys was investigated in an acidic brine... Keywords: Galvanic corrosion, carbon steel, nickel-rich and nickel-base alloys, titanium alloy, galvanic current. galvanic potential, temperature effect.
Galvanic corrosion behavior of A 5 16 steel separately coupled to six different corrosion-resistant alloys was investigated in an acidic brine... Keywords: Galvanic corrosion, carbon steel, nickel-rich and nickel-base alloys, titanium alloy, galvanic current. galvanic potential, temperature effect.
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for 98147 FACTORS INFLUENCING THE PERFORMANCE OF
Available for download

98147 FACTORS INFLUENCING THE PERFORMANCE OF CARBON STEEL OVERPACKS IN THE PROPOSED HIGH-LEVEL NUCLEAR WASTE REPOSITORY

Product Number: 51300-98147-SG
ISBN: 98147 1998 CP
Author: G.A. Cragnolino, D.S. Dunn, P. Angell, Y.M. Pan, N. Sridhar
$20.00
Picture for 98158 INITIATION CRITERIA FOR CREVICE CORROSION
Available for download

98158 INITIATION CRITERIA FOR CREVICE CORROSION OF TITANIUM ALLOYS USED FOR HLW DISPOSAL OVERPACK

Product Number: 51300-98158-SG
ISBN: 98158 1998 CP
Author: Masatsune Akashi, Guen Nakayama, Takanori Fukuda
$20.00
Picture for 98148 EFFECT OF GALVANIC COUPLING BETWEEN
Available for download

98148 EFFECT OF GALVANIC COUPLING BETWEEN OVERPACK MATERIALS FOR HIGH-LEVEL NUCLEAR WASTE CONTAINERS

Product Number: 51300-98148-SG
ISBN: 98148 1998 CP
Author: D.S. Dunn, G.A. Cragnolino, N. Sridhar
$20.00