96255 EFFECT OF STRESS CORROSION CRACKING ON INTEGRITY AND REMAINING LIFE OF NATURAL GAS PIPELINES

Product Number: 51300-96255-SG
ISBN: 96255 1996 CP
Author: C. E. Jaske, J. A. Beavers, B. A. Harle
$0.00
$20.00
$20.00
External stress-corrosion cracking of pipelines is a serious problem for the gm transmission industry. Longitudinal cracks initiate on the outside surface of the pipe and link up to form flaws that, in some cases, can lead to pipe rupture. This paper presents a model that quantities the effect of stress-corrosion cracking on pipe failure stress. The model is an extension of those that have been developed for oil and gas pipelines and considers both flow-stress and fracture toughness dependent failure modes. A methodology also is presented to calculate the remaining life of a pipeline containing flaws of known size. Keywords: pipelines, stress-conosion cracking, fracture mechanics, life assessment.
External stress-corrosion cracking of pipelines is a serious problem for the gm transmission industry. Longitudinal cracks initiate on the outside surface of the pipe and link up to form flaws that, in some cases, can lead to pipe rupture. This paper presents a model that quantities the effect of stress-corrosion cracking on pipe failure stress. The model is an extension of those that have been developed for oil and gas pipelines and considers both flow-stress and fracture toughness dependent failure modes. A methodology also is presented to calculate the remaining life of a pipeline containing flaws of known size. Keywords: pipelines, stress-conosion cracking, fracture mechanics, life assessment.
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for 96249 STRESS CORROSION CRACKING OF PIPELINES
Available for download

96249 STRESS CORROSION CRACKING OF PIPELINES - ITS CONTROL OR PREVENTION.

Product Number: 51300-96249-SG
ISBN: 96249 1996 CP
Author: R.N. Parkins
$20.00
Picture for 04189 Stress Corrosion Cracking Prediction Model
Available for download

04189 Stress Corrosion Cracking Prediction Model

Product Number: 51300-04189-SG
ISBN: 04189 2004 CP
Author: John A. Beavers and William V. Harper, CC Technologies; Richard McGregor, Great Lakes Gas Transmissi
$20.00
Picture for 00370 RESEARCH CHALLENGES REGARDING STRESS
Available for download

00370 RESEARCH CHALLENGES REGARDING STRESS-CORROSION CRACKING OF PIPELINES

Product Number: 51300-00370-SG
ISBN: 00370 2000 CP
Author: R. R. Fessler, K. Krist
$20.00