11423 Development of a Stress Corrosion Test Specimen for Determining the Stress Corrosion Resistance of Aluminum 5XXX Marine Alloys

Product Number: 51300-11423-SG
ISBN: 2011 11423 CP
Author: Thomas J. Summerson
Publication Date: 2011
$0.00
$20.00
$20.00
ASTM Task Group B07.03/G01.09 needed a stress corrosion test specimen for relating nitric acid mass losses (ASTM G67) cited in ASTM B928 to stress corrosion resistance in marine environments. ASTM B928 was established in 2004, following an inspection survey in 2002 of several boats exhibiting stress corrosion cracking in hull and deck plates of 5083-H321. (1) The intent of B928 is to prevent use of alloys and tempers that are not resistant to intergranular corrosion, exfoliation and stress corrosion. Resistant tempers cited in B928 are –H116 and –H321. This paper describes how a preform- stressed specimen configuration was found to serve this purpose. Results of Point Loma, CA. atmospheric test of preformed samples of sensitized 5083-H321 in both sheet and plate thicknesses are provided. This led to the ASTM Task Group’s current use of a modified perform specimen configuration (U-Bend) for more extensive SC tests of the 5XXX alloys with varying mass loss values.

ASTM Task Group B07.03/G01.09 needed a stress corrosion test specimen for relating nitric acid mass losses (ASTM G67) cited in ASTM B928 to stress corrosion resistance in marine environments. ASTM B928 was established in 2004, following an inspection survey in 2002 of several boats exhibiting stress corrosion cracking in hull and deck plates of 5083-H321. (1) The intent of B928 is to prevent use of alloys and tempers that are not resistant to intergranular corrosion, exfoliation and stress corrosion. Resistant tempers cited in B928 are –H116 and –H321. This paper describes how a preform- stressed specimen configuration was found to serve this purpose. Results of Point Loma, CA. atmospheric test of preformed samples of sensitized 5083-H321 in both sheet and plate thicknesses are provided. This led to the ASTM Task Group’s current use of a modified perform specimen configuration (U-Bend) for more extensive SC tests of the 5XXX alloys with varying mass loss values.

Product tags
Also Purchased
Picture for 11425 Development of Test Specimens for Evaluating SCC Behavior
Available for download

11425 Development of Test Specimens for Evaluating SCC Behavior of Marine Aluminum Alloys and Assessment of the Severity of Various Marine Exposure Conditions

Product Number: 51300-11425-SG
ISBN: 2011 11425 CP
Author: Francine Bovard, Jerry Curran, Christine Henon, Jim Towers, Rebecca Wyss, Jacob Padrul, C. Wong
Publication Date: 2011
$20.00
Picture for 08206 Correlation of Electrochemistry and ASTM Tests in the Corrosion Behavior of 5XXX Aluminum Allo
Available for download

08206 Correlation of Electrochemistry and ASTM Tests in the Corrosion Behavior of 5XXX Aluminum Alloys

Product Number: 51300-08206-SG
ISBN: 08206 2008 CP
Author: Elissa Bumiller and Robert Ruedisueli
Publication Date: 2008
$20.00
Picture for 09512 Correlation of Electrochemical, ASTM Test and Metallographic Annalyses in the Corrosion Behavi
Available for download

09512 Correlation of Electrochemical, ASTM Test and Metallographic Annalyses in the Corrosion Behavior of 5XXX Aluminum Alloys

Product Number: 51300-09512-SG
ISBN: 09512 2009 CP
Author: Robert Ruedisueli and Elissa Bumiller
Publication Date: 2009
$20.00