The failures of boiler tubes have consistently occurred in the Refinery (Ras Tanura, Jiddah and Riyadh) and gas plants (Ju’aymah and Shedgum). The Research and Development Center (R&DC) has helped the plant engineers to overcome the problems by identifying the nature and source of compounds (e.g., corrosion products, formation materials and scale deposits). The boiler consists of a furnace, boiler tubes, steam drum, mud drum and boiler. The furnace usually provides heat to the boiler and then changes water into steam. Here are the problems on why boiler tubes failed. The presence of vanadium and sodium compounds in the sample indicates the quality of burning fuels is poor. Also, if the large quantities of hematite-Fe2O3 (>15%) appears in the deposits, it indicates the presence of dissolved oxygen in boiler feed water. Additionally, if iron carbonate appears in the samples, it indicates the presence of dissolved carbon dioxide (CO2) in the system. Moreover, if the metallic copper is presence in the deposits, it indicates erosion in the boiler. Then, a special precaution to prevent the plating out of copper during cleaning operations is required. The identification procedures of the corrosion products, formation materials and scale deposit materials will be described.

Key words: Hematite, copper, boiler tubes, corrosion products, XRD
The failures of boiler tubes have consistently occurred in the Refinery (Ras Tanura, Jiddah and Riyadh) and gas plants (Ju’aymah and Shedgum). The Research and Development Center (R&DC) has helped the plant engineers to overcome the problems by identifying the nature and source of compounds (e.g., corrosion products, formation materials and scale deposits). The boiler consists of a furnace, boiler tubes, steam drum, mud drum and boiler. The furnace usually provides heat to the boiler and then changes water into steam. Here are the problems on why boiler tubes failed. The presence of vanadium and sodium compounds in the sample indicates the quality of burning fuels is poor. Also, if the large quantities of hematite-Fe2O3 (>15%) appears in the deposits, it indicates the presence of dissolved oxygen in boiler feed water. Additionally, if iron carbonate appears in the samples, it indicates the presence of dissolved carbon dioxide (CO2) in the system. Moreover, if the metallic copper is presence in the deposits, it indicates erosion in the boiler. Then, a special precaution to prevent the plating out of copper during cleaning operations is required. The identification procedures of the corrosion products, formation materials and scale deposit materials will be described.

Key words: Hematite, copper, boiler tubes, corrosion products, XRD
Product tags
Also Purchased
Picture for Problems and mitigation experiences with black powder inside of the long-distance natural gas pipeli
Available for download

51312-01589-Problems and mitigation experiences with black powder inside of the long-distance natural gas pipeli

Product Number: 51312-01589-SG
ISBN: 01589 2012 CP
Author: Zhang Peng
Publication Date: 2012
$20.00
Picture for 090560 Thermodynamic Analysis of the Formation of Black Powder in Sales Gas Pipelines
Available for download

090560 Thermodynamic Analysis of the Formation of Black Powder in Sales Gas Pipelines

Product Number: 51300-0090560-SG
ISBN: 090560 2009 CP
Author: Abdelmounam, M. Sherik and Boyd R. Davis
Publication Date: 2009
$20.00
Picture for 11086 Laboratory Simulation of Black Powder Formation in Flowing Gas with Water Condensation
Available for download

11086 Laboratory Simulation of Black Powder Formation in Flowing Gas with Water Condensation

Product Number: 51300-11086-SG
ISBN: 2011 11086 CP
Author: Gaute Svenningsen, Martin Foss, Rolf Nyborg, Abdelmounam M. Sherik and Arnold L. Lewis
Publication Date: 2011
$20.00