Search
Filters
Close

11264 Internal Pitting Corrosion of X80 Pipeline Steel under Deposited Sand Bed in CO2-Saturated

Product Number: 51300-11264-SG
ISBN: 2011 11264 CP
Author: Huibin Xue, Frank Y. Cheng, Zhenjin Zhu, Nima Tajallipour, Patrick J. Teevens
Publication Date: 2011
$0.00
$20.00
$20.00
Internal pitting corrosion of steel occurring under a layer of solid sands constitutes an essential threat to the integrity of the pipeline system in petroleum production. In this work, micro-electrochemical techniques, including localized electrochemical impedance spectroscopy and scanning vibrating electrode technique, were used to characterize in-situ the pitting corrosion processes of an X80 steel in CO2-saturated NaCl solutions. Results demonstrated that corrosion pits could initiate and grow on the steel, which is covered with a layer of sands. With the increase of test time, pits keep growing, resulting in a drop of local impedance and an increase of the peak current density. Moreover, the increase of chloride concentration in the solution and the solution flow velocity favors the growth of corrosion pits.

2 Keywords: Internal pitting corrosion, pipeline steel, sands, micro-electrochemical measurements
Internal pitting corrosion of steel occurring under a layer of solid sands constitutes an essential threat to the integrity of the pipeline system in petroleum production. In this work, micro-electrochemical techniques, including localized electrochemical impedance spectroscopy and scanning vibrating electrode technique, were used to characterize in-situ the pitting corrosion processes of an X80 steel in CO2-saturated NaCl solutions. Results demonstrated that corrosion pits could initiate and grow on the steel, which is covered with a layer of sands. With the increase of test time, pits keep growing, resulting in a drop of local impedance and an increase of the peak current density. Moreover, the increase of chloride concentration in the solution and the solution flow velocity favors the growth of corrosion pits.

2 Keywords: Internal pitting corrosion, pipeline steel, sands, micro-electrochemical measurements
Product tags
Also Purchased
Picture for 11266 Under Deposit Corrosion From Iron Sulfide
Available for download

11266 Under Deposit Corrosion From Iron Sulfide

Product Number: 51300-11266-SG
ISBN: 2011 11266 CP
Author: Sarah Standlee, K. Daniel Efird, Derek Spiller
Publication Date: 2011
$20.00
Picture for 11261 Inhibition of CO2 Corrosion of 1030 Carbon Steel Beneath Sand-Deposits
Available for download

11261 Inhibition of CO2 Corrosion of 1030 Carbon Steel Beneath Sand-Deposits

Product Number: 51300-11261-SG
ISBN: 2011 11261 CP
Author: Vedapriya Pandarinathan, Katerina Lepková and Rolf Gubner
Publication Date: 2011
$20.00
Picture for CO2 Corrosion and the Inhibitor Effectiveness Under Sand Deposit in Offshore Pipeline
Available for download

51314-4183-CO2 Corrosion and the Inhibitor Effectiveness Under Sand Deposit in Offshore Pipeline

Product Number: 51314-4183-SG
ISBN: 4183 2014 CP
Author: Wei Cui
Publication Date: 2014
$0.00