11115 Mitigation of Sulfide Stress Cracking in Down Hole P110 Components via Low Plasticity Burnishing

Product Number: 51300-11115-SG
ISBN: 11115 2011 CP
Author: Jeremy Scheel, Doug Hornbach, Paul Prevéy, Darrel Chelette, Peter Moore
Publication Date: 2011
$0.00
$20.00
$20.00
Sulfide stress cracking (SSC) along with hydrogen embrittlement (HE) prevents the use of less expensive high strength carbon steel alloys in the recovery of fossil fuels in H2S containing ‘sour’ service environments that are commonly seen in deep well fossil fuel recovery efforts. High magnitude tensile stresses are generated by connection interferences created during power make-up of down hole tubular components. When subject to service loads the stresses are increased further providing the high tensile stresses necessary for SSC initiation. Because these alloys processed into high strength grades are not suited for fully saturated sour service environments, the current solution is to use or develop much more expensive alloys with increased corrosion-cracking resistance or limit their use to significantly weaker sour environments or higher operating temperatures.

Introduction of stable, high magnitude compressive residual stresses into less expensive carbon steel alloys alleviates the tensile stresses and mitigates SSC while also improving fatigue strength. This could allow the potential of using less expensive alloys in sour environments. Low plasticity burnishing (LPB) is highly effective when applied to metallic components using a proven reproducible process of producing deep, high magnitude compressive residual stresses in complex geometric components without altering the geometry, design or chemistry.

The LPB process, applied with advanced control systems, is presently being employed to treat components resulting in a substantial increase in service life through SSC mitigation and improved fatigue life. The benefits of LPB have been evaluated on full size specimens of uni-axial hoop stress loaded coupling blanks and C-ring specimens manufactured from quench and tempered API P110 grade steel with a yield strength of 132 ksi (910 MPa). Specimens were exposed to 100% NACE TM0177-Solution A at 1 bara H2S in both the LPB treated and untreated condition. The time to failure was documented along with the increase in life resulting from LPB treatment. LPB was successful in completely mitigating SSC in each test specimen up to 85% SMYS hoop tension; and in each case met or exceeded the 720-hour exposure time defined in NACE TM0177. At an applied fiber stress of 90% SMYS, the C-ring samples have exceeded exposures of 840 hours without failure. The initial results indicate that LPB processing of down hole tubular components may provide an alternative economical means of SSC mitigation and greatly reducing risk of component failure in sour environments.

Key Words: low plasticity burnishing, sulfide stress cracking, fatigue, residual stress, sour service
Sulfide stress cracking (SSC) along with hydrogen embrittlement (HE) prevents the use of less expensive high strength carbon steel alloys in the recovery of fossil fuels in H2S containing ‘sour’ service environments that are commonly seen in deep well fossil fuel recovery efforts. High magnitude tensile stresses are generated by connection interferences created during power make-up of down hole tubular components. When subject to service loads the stresses are increased further providing the high tensile stresses necessary for SSC initiation. Because these alloys processed into high strength grades are not suited for fully saturated sour service environments, the current solution is to use or develop much more expensive alloys with increased corrosion-cracking resistance or limit their use to significantly weaker sour environments or higher operating temperatures.

Introduction of stable, high magnitude compressive residual stresses into less expensive carbon steel alloys alleviates the tensile stresses and mitigates SSC while also improving fatigue strength. This could allow the potential of using less expensive alloys in sour environments. Low plasticity burnishing (LPB) is highly effective when applied to metallic components using a proven reproducible process of producing deep, high magnitude compressive residual stresses in complex geometric components without altering the geometry, design or chemistry.

The LPB process, applied with advanced control systems, is presently being employed to treat components resulting in a substantial increase in service life through SSC mitigation and improved fatigue life. The benefits of LPB have been evaluated on full size specimens of uni-axial hoop stress loaded coupling blanks and C-ring specimens manufactured from quench and tempered API P110 grade steel with a yield strength of 132 ksi (910 MPa). Specimens were exposed to 100% NACE TM0177-Solution A at 1 bara H2S in both the LPB treated and untreated condition. The time to failure was documented along with the increase in life resulting from LPB treatment. LPB was successful in completely mitigating SSC in each test specimen up to 85% SMYS hoop tension; and in each case met or exceeded the 720-hour exposure time defined in NACE TM0177. At an applied fiber stress of 90% SMYS, the C-ring samples have exceeded exposures of 840 hours without failure. The initial results indicate that LPB processing of down hole tubular components may provide an alternative economical means of SSC mitigation and greatly reducing risk of component failure in sour environments.

Key Words: low plasticity burnishing, sulfide stress cracking, fatigue, residual stress, sour service
Product tags
Also Purchased
Picture for 11105 Sulfide Stress Cracking Susceptibility of Local Hard Areas in Carbon Steel Weld Heat Affected
Available for download

11105 Sulfide Stress Cracking Susceptibility of Local Hard Areas in Carbon Steel Weld Heat Affected

Product Number: 51300-11105-SG
ISBN: 11105 2011 CP
Author: Ben Crowder, James Buchanan, Sam Mishael, and Ron Shockley
Publication Date: 2011
$20.00
Picture for 11107 Effect of Residual Stresses on the HIC Resistance of ERW Pipes and Line Pipe Applications
Available for download

11107 Effect of Residual Stresses on the HIC Resistance of ERW Pipes and Line Pipe Applications

Product Number: 51300-11107-SG
ISBN: 11107 2011 CP
Author: J. Kraegeloh, C. Bosch, H. Brauer, A. Kulgemeyer
Publication Date: 2011
$20.00
Picture for 11100 Environmentally Assisted Cracking Testing of High Strength 15Cr Steel in Sour Well Environment
Available for download

11100 Environmentally Assisted Cracking Testing of High Strength 15Cr Steel in Sour Well Environments

Product Number: 51300-11100-SG
ISBN: 11100 2011 CP
Author: John Meng, Brian Chambers, Russell D. Kane, Jim Skogsberg, Mitsuo Kimura and Ken Shimamoto
Publication Date: 2011
$20.00