10344 Localized Corrosion Resistance of UNS S32750 and UNS S33207 Duplex Umbilical Tubes in Synthetic Seawater

Product Number: 51300-10344-SG
ISBN: 10344 2010 CP
Author: John Meng, Adeyinka Adeleke and Sean Derrickson
Publication Date: 2010
$0.00
$20.00
$20.00
The resistance to localized corrosion of girth-welded UNS S32750 and UNS S33207 duplex stainless steel umbilical tubes in synthetic seawater at different temperatures was investigated using electrochemical methods, such as cyclic potentiodynamic polarization (CPP) and potentiostatic polarization, and long-term immersion tests. Repassivation potentials as determined from the CPP tests were compared with the open-circuit potential (OCP) obtained from the long-term immersion tests to address the long-term localized corrosion resistance of umbilical tubes. Electrochemical results indicate that the critical pitting temperature (CPT) for the welded S32750 and S33207 tubes were 53°C and 68°C, respectively. The critical crevice temperature (CCT) for both welded tubes was similar to the CPT values. Interestingly, despite the critical temperatures mentioned above, the 45-day immersion tests show no pitting or crevice corrosion for the welded S32750 tubes at temperatures of 50~70°C and the welded S33207 tubes at temperatures of 60~80°C in aerated synthetic seawater.

Keywords: duplex stainless steel, localized corrosion, umbilical, synthetic seawater
The resistance to localized corrosion of girth-welded UNS S32750 and UNS S33207 duplex stainless steel umbilical tubes in synthetic seawater at different temperatures was investigated using electrochemical methods, such as cyclic potentiodynamic polarization (CPP) and potentiostatic polarization, and long-term immersion tests. Repassivation potentials as determined from the CPP tests were compared with the open-circuit potential (OCP) obtained from the long-term immersion tests to address the long-term localized corrosion resistance of umbilical tubes. Electrochemical results indicate that the critical pitting temperature (CPT) for the welded S32750 and S33207 tubes were 53°C and 68°C, respectively. The critical crevice temperature (CCT) for both welded tubes was similar to the CPT values. Interestingly, despite the critical temperatures mentioned above, the 45-day immersion tests show no pitting or crevice corrosion for the welded S32750 tubes at temperatures of 50~70°C and the welded S33207 tubes at temperatures of 60~80°C in aerated synthetic seawater.

Keywords: duplex stainless steel, localized corrosion, umbilical, synthetic seawater
Product tags
Also Purchased
Picture for 11349 Chemical Induced Pitting Corrosion Of Super Duplex Stainless Steel Umbilical Tubes
Available for download

11349 Chemical Induced Pitting Corrosion Of Super Duplex Stainless Steel Umbilical Tubes

Product Number: 51300-11349-SG
ISBN: 2011 11349 CP
Author: Heider A. Suarez, Robert J. Franco, William E. Bond and Raju S. Pakalapati
Publication Date: 2011
$20.00
Picture for Super Duplex Stainless Steel Welded Tubes: an innovative solution for offshore umbilicals
Available for download

51312-01658-Super Duplex Stainless Steel Welded Tubes: an innovative solution for offshore umbilicals

Product Number: 51312-01658-SG
ISBN: 01658 2012 CP
Author: Hafida El Alami
Publication Date: 2012
$20.00
Picture for 10342 Properties of a New Lean Duplex Alloy
Available for download

10342 Properties of a New Lean Duplex Alloy

Product Number: 51300-10342-SG
ISBN: 10342 2010 CP
Author: John F. Grubb, Bahri Ozturk, David S. Bergstrom, and John J. Dunn
Publication Date: 2010
$20.00