Search
Filters
Close

09463 Applying ASTM G71 to Galvanic Corrosion Testing of Small Medical Implants

Product Number: 51300-09463-SG
ISBN: 09463 2009 CP
Author: Bradley D. Krantz
Publication Date: 2009
$0.00
$20.00
$20.00
Screening tests to qualify materials for modern medical devices and implants are necessary to ensure longevity of service with minimal risk of failure by electrochemical (corrosion) or mechanical causes. New devices and medical procedures that involve placing different materials in direct contact with each other may be prone to localized galvanic corrosion, the propensity for which could be identified by using suitable laboratory testing. ASTM G71, which was developed for the chemical and process industries, can be applied to provide indications for small medical devices used in-vivo. This paper describes the laboratory testing procedures and provides some representative examples pertinent to medical implants.

Keywords: galvanic corrosion, medical devices, nitinol, ASTM G71
Screening tests to qualify materials for modern medical devices and implants are necessary to ensure longevity of service with minimal risk of failure by electrochemical (corrosion) or mechanical causes. New devices and medical procedures that involve placing different materials in direct contact with each other may be prone to localized galvanic corrosion, the propensity for which could be identified by using suitable laboratory testing. ASTM G71, which was developed for the chemical and process industries, can be applied to provide indications for small medical devices used in-vivo. This paper describes the laboratory testing procedures and provides some representative examples pertinent to medical implants.

Keywords: galvanic corrosion, medical devices, nitinol, ASTM G71
Product tags
Also Purchased
Picture for 09461 Pitting Resistance of Nitinol Stents Before and After Implantation
Available for download

09461 Pitting Resistance of Nitinol Stents Before and After Implantation

Product Number: 51300-09461-SG
ISBN: 09461 2009 CP
Author: Robert Cannon and Lorrie A. Krebs
Publication Date: 2009
$20.00
Picture for 09464 Accelerated Testing of Active Implantable Medical Devices
Available for download

09464 Accelerated Testing of Active Implantable Medical Devices

Product Number: 51300-09464-SG
ISBN: 09464 2009 CP
Author: Larry Eiselstein, Paul Verghese and Eric P. Guyer
Publication Date: 2009
$20.00
Picture for 09466 Corrosion and Immune Response of Advanced Titanium Alloys In Biological Environments
Available for download

09466 Corrosion and Immune Response of Advanced Titanium Alloys In Biological Environments

Product Number: 51300-09466-SG
ISBN: 09466 2009 CP
Author: V .Ravi; G. Rey; D. Miracle; K. Morin; S. Castaneda; S. Tamirisa; W. Wantah; B. Permana and S. Alas
Publication Date: 2009
$20.00