08495 A Multi-Scale Approach to Stress Corrosion Cracking Characterization

Product Number: 51300-08495-SG
ISBN: 08495 2008 CP
Author: Sergio Lozano-Perez
Publication Date: 2008
$0.00
$20.00
$20.00
A multi-scale approach to stress corrosion cracking has been applied to 304 type stainless steels and it is presented in this paper. The influence of cold work and chromium concentration in the alloy has been characterized. It will be shown that the same crack and, more importantly, the crack tip region can be characterized with surface techniques such as NanoSIMS and EBSD and later prepared for TEM. This will offer a unique insight into the chemistry and microstructure, proving that the right combination of techniques can provide most of the information needed to correctly understand the mechanisms of crack propagation.
A multi-scale approach to stress corrosion cracking has been applied to 304 type stainless steels and it is presented in this paper. The influence of cold work and chromium concentration in the alloy has been characterized. It will be shown that the same crack and, more importantly, the crack tip region can be characterized with surface techniques such as NanoSIMS and EBSD and later prepared for TEM. This will offer a unique insight into the chemistry and microstructure, proving that the right combination of techniques can provide most of the information needed to correctly understand the mechanisms of crack propagation.
Product tags
Also Purchased
Picture for 96249 STRESS CORROSION CRACKING OF PIPELINES
Available for download

96249 STRESS CORROSION CRACKING OF PIPELINES - ITS CONTROL OR PREVENTION.

Product Number: 51300-96249-SG
ISBN: 96249 1996 CP
Author: R.N. Parkins
$20.00
Picture for 08492 Effects of Temperature and Humidity on Atmospheric Stress Corrosion Cracking of 304 Stainless
Available for download

08492 Effects of Temperature and Humidity on Atmospheric Stress Corrosion Cracking of 304 Stainless Steel

Product Number: 51300-08492-SG
ISBN: 08492 2008 CP
Author: Hitoshi Hayashibara, Masami Mayuzumi, Yoshihiro Mizutani, and Jun-ichi Tani
Publication Date: 2008
$20.00
Picture for 08500 The Influence of Weld Heat-Affected Zone on Stress Corrosion Cracking of Pipeline Steel in Nea
Available for download

08500 The Influence of Weld Heat-Affected Zone on Stress Corrosion Cracking of Pipeline Steel in Near-Neutral pH Environment

Product Number: 51300-08500-SG
ISBN: 08500 2008 CP
Author: B. Fang, E. Han, J. Wang, W. Ke, R. Eadie, W. Zheng, M. Elboujdaini, and W. Revie
Publication Date: 2008
$20.00