08325 Laboratory Evaluation and Modeling of API-L80/13Cr Galvanic Corrosion in CO2 Environment

Product Number: 51300-08325-SG
ISBN: 08325 2008 CP
Author: Conchita Mendez and Colin Scott
Publication Date: 2008
$0.00
$20.00
$20.00
A laboratory evaluation was performed to assess the galvanic coupling corrosion of API L-80 carbon steel coupled with 13Cr in sodium chloride solution at 30 and 80°C and 100 psi of carbon dioxide (CO2). Electrochemical techniques where used (linear polarization and potentiodynamic polarization) with the un-coupled materials. Also the mixed potential and galvanic current change with time were measured after coupling using a zero resistance ammeter (ZRA). Two anode/cathode ratios were used (1:1 and 1:2). Some electrochemical impedance tests were done to determine the electrolyte resistance. Finite element (FE) analyses were also attempted to predict the extent and distribution of galvanic corrosion simulating two geometries (laboratory assembly and pipeline of different lengths).
A laboratory evaluation was performed to assess the galvanic coupling corrosion of API L-80 carbon steel coupled with 13Cr in sodium chloride solution at 30 and 80°C and 100 psi of carbon dioxide (CO2). Electrochemical techniques where used (linear polarization and potentiodynamic polarization) with the un-coupled materials. Also the mixed potential and galvanic current change with time were measured after coupling using a zero resistance ammeter (ZRA). Two anode/cathode ratios were used (1:1 and 1:2). Some electrochemical impedance tests were done to determine the electrolyte resistance. Finite element (FE) analyses were also attempted to predict the extent and distribution of galvanic corrosion simulating two geometries (laboratory assembly and pipeline of different lengths).
Product tags
Also Purchased
Picture for 00152 CORROSION PERFORMANCE OF 13CR STAINLESS
Available for download

00152 CORROSION PERFORMANCE OF 13CR STAINLESS STEELS

Product Number: 51300-00152-SG
ISBN: 00152 2000 CP
Author: Trond Rogne, John M. Drugli, Ole Oystein Knudsen, Stein Olsen and Jakob Enerhaug
$20.00
Picture for 08332 Roles of Passivation and Galvanic Effects in Localized CO2 Corrosion of Mild Steel
Available for download

08332 Roles of Passivation and Galvanic Effects in Localized CO2 Corrosion of Mild Steel

Product Number: 51300-08332-SG
ISBN: 08332 2008 CP
Author: Jiabin Han, Yang Yang, Srdjan Nesic, and Bruce N. Brown
Publication Date: 2008
$20.00
Picture for 97039 LIMITATIONS FOR THE APPLICATION
Available for download

97039 LIMITATIONS FOR THE APPLICATION OF 13CR STEEL IN OIL AND GAS Production ENVIRONMENTS

Product Number: 51300-97039-SG
ISBN: 97039 1997 CP
Author: Sytze Huizinga, W. E. Liek
$20.00