08256 Localized Corrosion of a Super-Austenitic Stainless Steel (Fe-24Ni-20Cr-6.3Mo-0.22N) Brazed with a Ni-based braze (Ni-22Cr-6.3Si-3.8P): Effect of Braze Clearance on Corrosion Resistance

Product Number: 51300-08256-SG
ISBN: 08256 2008 CP
Author: Joshua James, John Scully, and Jim Fitz-Gerald
Publication Date: 2008
$0.00
$20.00
$20.00
The microstructural and local corrosion characteristics of a super-austenitic stainless steel (SASS), (Fe-24Ni-20.5Cr-6.3Mo-0.22N, UNS N08367), brazed with a commercially available Ni-based filler alloy, (Ni-22Cr-6.5Si-3.5P) are investigated. The isolated SASS base material is intrinsically resistant to pitting and crevice corrosion in 0.6 M NaCl solution at room temperature. Isolated braze alloy, tested as a bead prepared at 1150 °C for 60 minutes in a vacuum furnace, without the diffusive egress of melting point depressants (MPDs) exhibited critical potentials for localized corrosion in 0.6 M NaCl well below that of the SASS. This is due to both the low pitting resistance equivalency number (PREN) of the Ni-Cr solid solution and the loss of beneficial Cr due to formation of silicide and phosphide phases, enabled by the presence of these MPDs.
The microstructural and local corrosion characteristics of a super-austenitic stainless steel (SASS), (Fe-24Ni-20.5Cr-6.3Mo-0.22N, UNS N08367), brazed with a commercially available Ni-based filler alloy, (Ni-22Cr-6.5Si-3.5P) are investigated. The isolated SASS base material is intrinsically resistant to pitting and crevice corrosion in 0.6 M NaCl solution at room temperature. Isolated braze alloy, tested as a bead prepared at 1150 °C for 60 minutes in a vacuum furnace, without the diffusive egress of melting point depressants (MPDs) exhibited critical potentials for localized corrosion in 0.6 M NaCl well below that of the SASS. This is due to both the low pitting resistance equivalency number (PREN) of the Ni-Cr solid solution and the loss of beneficial Cr due to formation of silicide and phosphide phases, enabled by the presence of these MPDs.
Product tags
Also Purchased
Picture for 08257 Corrosion of A Super-Austenitic Stainless Steel (Fe-24Ni-20Cr-6.3Mo-0.22N) When Brazed with a
Available for download

08257 Corrosion of A Super-Austenitic Stainless Steel (Fe-24Ni-20Cr-6.3Mo-0.22N) When Brazed with a Ni-Cr Braze Material (Ni-22Cr-6.3Si-3.8P): Corrosion Behavior of Isolated and Combined Materials

Product Number: 51300-08257-SG
ISBN: 08257 2008 CP
Author: Sara Hebb, Joshua James, Jim Gerald, George Young, and John Scully
Publication Date: 2008
$20.00
Picture for 08237 Corrosion Resistance of Si and Al Bearing Ultrafine Grained Weathering Steel in the Saline Atm
Available for download

08237 Corrosion Resistance of Si and Al Bearing Ultrafine Grained Weathering Steel in the Saline Atmosphere

Product Number: 51300-08237-SG
ISBN: 08237 2008 CP
Author: Toshiyasu Nishimura and Sengodan Tamilselvi
Publication Date: 2008
$20.00
Picture for 08248 Crevice Corrosion Evaluation of UNS N08367 Welds Applied by Different Welding Techniques
Available for download

08248 Crevice Corrosion Evaluation of UNS N08367 Welds Applied by Different Welding Techniques

Product Number: 51300-08248-SG
ISBN: 08248 2008 CP
Author: Theresa Newbauer, Edward Lemieux, Kunigahalli Vasanth, and Kimngoc Tran
Publication Date: 2008
$20.00