08229 Galvanic Corrosion Performance of High Strength Copper-Nickel Alloys in Seawater

Product Number: 51300-08229-SG
ISBN: 08229 2008 CP
Author: J. Wharton, R. Barik, R. Wood, and K. Stokes
Publication Date: 2008
$0.00
$20.00
$20.00
High strength copper-nickel (Cu-Ni-Mn-Al-Nb) alloys are widely used for marine applications due to their excellent resistance to seawater corrosion, high inherent resistance to biofouling and ease of fabrication. However, in-service experience has shown that these alloys may encounter variable performance worldwide due to local environmental conditions. In particular, the corrosion performance of high strength Cu-Ni alloys may be affected by the seawater environmental factors, which include biofouling, temperature, salinity, pH and dissolved oxygen content. This study reports an investigation into the galvanic corrosion performance between two wrought high strength copper-nickel alloys, with nickel contents of 15 and 19 %, regarding the influence of surface oxide films / deposits and biofouling. X-ray photoelectron spectroscopy was used to study the composition of the corrosion product films. Analyses of galvanic currents, coupled and decoupled potentials routinely monitored for seawater immersion over a period of 2 years are presented.
High strength copper-nickel (Cu-Ni-Mn-Al-Nb) alloys are widely used for marine applications due to their excellent resistance to seawater corrosion, high inherent resistance to biofouling and ease of fabrication. However, in-service experience has shown that these alloys may encounter variable performance worldwide due to local environmental conditions. In particular, the corrosion performance of high strength Cu-Ni alloys may be affected by the seawater environmental factors, which include biofouling, temperature, salinity, pH and dissolved oxygen content. This study reports an investigation into the galvanic corrosion performance between two wrought high strength copper-nickel alloys, with nickel contents of 15 and 19 %, regarding the influence of surface oxide films / deposits and biofouling. X-ray photoelectron spectroscopy was used to study the composition of the corrosion product films. Analyses of galvanic currents, coupled and decoupled potentials routinely monitored for seawater immersion over a period of 2 years are presented.
Product tags
Also Purchased
Picture for 00627 COPPER-NICKEL ALLOYS FOR SEAWATER
Available for download

00627 COPPER-NICKEL ALLOYS FOR SEAWATER CORROSION RESISTANCE AND ANTIFOULING-A STATE OF THE ART REVIEW

Product Number: 51300-00627-SG
ISBN: 00627 2000 CP
Author: C.A.Powell, H.T. Michels
$20.00
Picture for 08231 Effect of Seawater Chlorination on the Erosion Corrosion Behaviour of Copper-Nickel Alloy CuNi
Available for download

08231 Effect of Seawater Chlorination on the Erosion Corrosion Behaviour of Copper-Nickel Alloy CuNi 90/10

Product Number: 51300-08231-SG
ISBN: 08231 2008 CP
Author: Wilhelm Schleich, Gunter Schmitt, Ralf Feser, Kathrin Schnier, Tim Gommlich, and Steffen Günther
Publication Date: 2008
$20.00