07587 Investigation of Crevice Corrosion of AISI 316 Stainless Steel and Ni-Cr-Mo Alloy 625 Using Coupled Multi-Electrode Arrays

Product Number: 51300-07587-SG
ISBN: 07587 2007 CP
Author: Florent Bocher, Noah D. Budiansky, John R. Scully, and Francisco Presuel-Moreno
Publication Date: 2007
$0.00
$20.00
$20.00
Close packed coupled multi-electrodes arrays (MEA) simulating a planar electrode were used to measure the anodic current evolution as a function of position during initiation and propagation of crevice corrosion of AISI 316 stainless steel (UNS S31600) and Ni-Cr-Mo alloy 625 (UNS N06625). Scaling laws derived from polarization data guided the implementation of rescaled crevices providing spatial resolution. Crevice corrosion of AISI 316 stainless steel in 0.6 M NaCl at 50°C was found to readily initiate close to the crevice mouth (i.e., xcrit ˜ 0) at modest applied potentials (e.g., Eapp=0 VSCE) and to spread inwards and outside the crevice with time. In the case of alloy 625, crevice corrosion initiates further inside the crevice (i.e., xcrit is large) and requires higher applied potential (e.g., Eapp=50 VSCE). The local crevice current density increased dramatically over a short period to reach a limiting value in both cases. The ramification of the larger critical depth for Ni-Cr-Mo alloys towards crevice corrosion susceptibility is also discussed.
Close packed coupled multi-electrodes arrays (MEA) simulating a planar electrode were used to measure the anodic current evolution as a function of position during initiation and propagation of crevice corrosion of AISI 316 stainless steel (UNS S31600) and Ni-Cr-Mo alloy 625 (UNS N06625). Scaling laws derived from polarization data guided the implementation of rescaled crevices providing spatial resolution. Crevice corrosion of AISI 316 stainless steel in 0.6 M NaCl at 50°C was found to readily initiate close to the crevice mouth (i.e., xcrit ˜ 0) at modest applied potentials (e.g., Eapp=0 VSCE) and to spread inwards and outside the crevice with time. In the case of alloy 625, crevice corrosion initiates further inside the crevice (i.e., xcrit is large) and requires higher applied potential (e.g., Eapp=50 VSCE). The local crevice current density increased dramatically over a short period to reach a limiting value in both cases. The ramification of the larger critical depth for Ni-Cr-Mo alloys towards crevice corrosion susceptibility is also discussed.
Product tags
Also Purchased
Picture for 02213 THE INFLUENCE OF ENVIRONMENTAL FACTORS...
Available for download

02213 THE INFLUENCE OF ENVIRONMENTAL FACTORS ON THE CREVICE CORROSION OF ALLOY 625 IN NATURAL SEAWATER

Product Number: 51300-02213-SG
ISBN: 02213 2002 CP
Author: F. J. Martin, P. M. Natishan, K. E. Lucas, E. A. Hogan, A. M. Grolleau, and E. D. Thomas
$20.00
Picture for Electrochemical Behavior of Passive Film Formed on Ni-Cr-Mo Alloy 625 in Neutral Sodium Chloride Sol
Available for download

51312-01319-Electrochemical Behavior of Passive Film Formed on Ni-Cr-Mo Alloy 625 in Neutral Sodium Chloride Sol

Product Number: 51312-01319-SG
ISBN: 01319 2012 CP
Author: Navid Attarzadeh
Publication Date: 2012
$20.00
Picture for 00182 COMPARISON OF THE CREVICE CORROSION
Available for download

00182 COMPARISON OF THE CREVICE CORROSION RESISTANCE OF ALLOYS 625 AND 22 IN CONCENTRATED CHLORIDE SOLUTION FROM 60 TO 95°C

Product Number: 51300-00182-SG
ISBN: 00182 2000 CP
Author: B.A. Kehler, G.O. Ilevbare, J.R. Scully