Metallurgical examinations were conducted on a set of damaged high alloy (Type 310H stainless steel and Alloy 625 weld overlay) superheater tubes removed from a coastal fluidized bed biomass power boiler, to better understand the degradation mode. Active oxidation (gas-solid reaction occurring underneath the chloride-containing fireside deposit) was found to be the mechanism responsible for the significant loss in tube wall thickness observed on damaged superheater tubes. There exists a complex, poorly-understood, synergy between the critical factors that affect active oxidation, primarily tube temperature and the supply of reactants in the flue gas, namely sodium chloride (NaCl), sulphur dioxide (SO2) and water vapour (H2O). Overall ranking in terms of increasing corrosion resistance to active oxidation follows the expected trend: T22 < SS310H < A625WO. Despite the favourable ranking, the Alloy 625 weld overlay can corrode by active oxidation at an appreciable rate [0.45 mm/yr (18 mpy)] under existing boiler operating conditions. A promising corrosion control strategy involves reducing the steam temperatures in the outlet tubes of the three superheater sections to below 500 °C.
Metallurgical examinations were conducted on a set of damaged high alloy (Type 310H stainless steel and Alloy 625 weld overlay) superheater tubes removed from a coastal fluidized bed biomass power boiler, to better understand the degradation mode. Active oxidation (gas-solid reaction occurring underneath the chloride-containing fireside deposit) was found to be the mechanism responsible for the significant loss in tube wall thickness observed on damaged superheater tubes. There exists a complex, poorly-understood, synergy between the critical factors that affect active oxidation, primarily tube temperature and the supply of reactants in the flue gas, namely sodium chloride (NaCl), sulphur dioxide (SO2) and water vapour (H2O). Overall ranking in terms of increasing corrosion resistance to active oxidation follows the expected trend: T22 < SS310H < A625WO. Despite the favourable ranking, the Alloy 625 weld overlay can corrode by active oxidation at an appreciable rate [0.45 mm/yr (18 mpy)] under existing boiler operating conditions. A promising corrosion control strategy involves reducing the steam temperatures in the outlet tubes of the three superheater sections to below 500 °C.
Product tags
Also Purchased
Picture for 07348 Issues Impacting Refractory Service Life in Biomass/Waste Gasification
Available for download

07348 Issues Impacting Refractory Service Life in Biomass/Waste Gasification

Product Number: 51300-07348-SG
ISBN: 07348 2007 CP
Author: James Bennett, Jasper Kwong, and Cindy Powell
Publication Date: 2007
$20.00
Picture for 07352 Contribution of Nickel Alloys in Solving Aqueous and High Temperature Corrosion Problems in In
Available for download

07352 Contribution of Nickel Alloys in Solving Aqueous and High Temperature Corrosion Problems in Incinerators and Vitrification/Management of Nuclear Waste

Product Number: 51300-07352-SG
ISBN: 07352 2007 CP
Author: Dinesh C. Agarwal
Publication Date: 2007
$20.00
Picture for 02379 SUPERHEATER CORROSION IN BIOMASS-FIRED...
Available for download

02379 SUPERHEATER CORROSION IN BIOMASS-FIRED POWER PLANTS: INVESTIGATION OF WELDS

Product Number: 51300-02379-SG
ISBN: 02379 2002 CP
Author: M. Montgomery, B. Carlsen, O. Biede, and O.H. Larsen
$20.00