$20.00
Seamless tubes type EN 1.4404 produced by hot extrusion have been internally electropolished at a mill that normally produces such tubes from welded tubes made from rolled plate. One or two standard passes have been applied. The short-range surface irregularities are removed by the electropolish, but the long-range waviness, and with that also the Ra value, remains unaffected by the electropolishing. The pitting resistance was evaluated by measurement of pitting potentials in solutions containing 500, 5000, and 50.000 mg/L chloride and temperatures from 10 to 95°C and by the ASTM G150 test. The asextruded and the once electropolished surfaces have pitting resistance very close to that observed with a rolled and pickled surface. The twice electropolished surface mostly have a much improved pitting resistance, but a few of the test results are no better than the parent material; this is discussed in terms of the number of pit initiation sites.
Seamless tubes type EN 1.4404 produced by hot extrusion have been internally electropolished at a mill that normally produces such tubes from welded tubes made from rolled plate. One or two standard passes have been applied. The short-range surface irregularities are removed by the electropolish, but the long-range waviness, and with that also the Ra value, remains unaffected by the electropolishing. The pitting resistance was evaluated by measurement of pitting potentials in solutions containing 500, 5000, and 50.000 mg/L chloride and temperatures from 10 to 95°C and by the ASTM G150 test. The asextruded and the once electropolished surfaces have pitting resistance very close to that observed with a rolled and pickled surface. The twice electropolished surface mostly have a much improved pitting resistance, but a few of the test results are no better than the parent material; this is discussed in terms of the number of pit initiation sites.
Product tags
Also Purchased
Picture for 07193 Rouging of Stainless Steel in WFI Systems - Examples and Present Understanding
Available for download

07193 Rouging of Stainless Steel in WFI Systems - Examples and Present Understanding

Product Number: 51300-07193-SG
ISBN: 07193 2007 CP
Author: Troels Mathiesen and Jan Elkjaer Frantsen
Publication Date: 2007
$20.00
Picture for 07196 Pitting Corrosion Problems of Stainless Steels in a PTA Plant
Available for download

07196 Pitting Corrosion Problems of Stainless Steels in a PTA Plant

Product Number: 51300-07196-SG
ISBN: 07196 2007 CP
Author: Oluwatoyin Ashiru and Abdullah Al-Refaie
Publication Date: 2007