A phenomenon that regularly plagues the standard austenitic stainless steels of type AISI 304/316 is stress-corrosion cracking (SCC). This paper discusses various cases of SCC and Stress Induced Cracking(SIC) that normally occur with austenitic stainless steel in fertilizer plants and describes three case studies. Chloride contamination (attack) is the main reason of SCC in different media such as steam, DM water and insulation (atmospheric corrosion). Guidelines of this paper may be useful for solving chloride - induced cracking and stress induced cracking in fertilizer plant. Key Words: Chloride stress corrosion cracking (CSCC), austenitic stainless steel, fertilizer, Demineralized (DM), chloride- induced cracking, Intergranular Stress(Strain) Induced Cracking (IGSIC), Yransgranular SCC (TGSCC), Corrosion Under Insulation (CUI). Part Per Million (PPM), Urea Grade (U.G).
A phenomenon that regularly plagues the standard austenitic stainless steels of type AISI 304/316 is stress-corrosion cracking (SCC). This paper discusses various cases of SCC and Stress Induced Cracking(SIC) that normally occur with austenitic stainless steel in fertilizer plants and describes three case studies. Chloride contamination (attack) is the main reason of SCC in different media such as steam, DM water and insulation (atmospheric corrosion). Guidelines of this paper may be useful for solving chloride - induced cracking and stress induced cracking in fertilizer plant. Key Words: Chloride stress corrosion cracking (CSCC), austenitic stainless steel, fertilizer, Demineralized (DM), chloride- induced cracking, Intergranular Stress(Strain) Induced Cracking (IGSIC), Yransgranular SCC (TGSCC), Corrosion Under Insulation (CUI). Part Per Million (PPM), Urea Grade (U.G).
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for 02439 EXTERNAL SCC PHENOMENA OF AUSTENITIC...
Available for download

02439 EXTERNAL SCC PHENOMENA OF AUSTENITIC STEEL IN UREA PLANTS STAINLESS

Product Number: 51300-02439-SG
ISBN: 02439 2002 CP
Author: A.H. Faraji
$20.00
Picture for 96232 Corrosion Inhibitors in Fertilizer
Available for download

96232 Corrosion Inhibitors in Fertilizer Production and Handling

Product Number: 51300-96232-SG
ISBN: 96232 1996 CP
Author: Prof. G.V. Prabhu-Gaurtkar, Prof A. Raman
$20.00
Picture for 99376 Advanced Water Resource Management in
Available for download

99376 Advanced Water Resource Management in Ammonia and Fertilizer Industries

Product Number: 51300-99376-SG
ISBN: 99376 1999 CP
Author: W. Hugh Goodman, Caries Campmajo
$20.00