Evidence for strength degradation of polycrystalline oxide fibers by stress corrosion from coating decomposition products is reviewed. More data on Strength degradation during fiber coating is presented. Models for stress corrosion are applied and discussed. The stress that drives corrosion is most likely thermal residual stress between grains in the polycrystalline fibers. The observed temperature dependence of stress corrosion is too strong to be controlled by bulk gas diffusion or Knudsen diffusion, but is consistent with control by strongly adsorbed surface active species.
Evidence for strength degradation of polycrystalline oxide fibers by stress corrosion from coating decomposition products is reviewed. More data on Strength degradation during fiber coating is presented. Models for stress corrosion are applied and discussed. The stress that drives corrosion is most likely thermal residual stress between grains in the polycrystalline fibers. The observed temperature dependence of stress corrosion is too strong to be controlled by bulk gas diffusion or Knudsen diffusion, but is consistent with control by strongly adsorbed surface active species.
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for 02415 FURTHER ADVANCES OF ENVIRONMENTALLY...
Available for download

02415 FURTHER ADVANCES OF ENVIRONMENTALLY FRIENDLY CORROSION INHIBITORS FOR CO2 CORROSION IN NORTH SEA OIL FIELDS

Product Number: 51300-02415-SG
ISBN: 02415 2002 CP
Author: Nihal Obeyesekere, Ali Naraghi, and Shelley Zhou
$20.00
Picture for 02414 A REVIEW ON MILD STEEL CORROSION...
Available for download
Picture for 02419 Measurement and Modeling of...
Available for download

02419 Measurement and Modeling of Environmentally Assisted Cracking of High-Temperature SiC/SiC Composites

Product Number: 51300-02419-SG
ISBN: 02419 2002 CP
Author: R.H. Jones, C.H. Henager, C.A. Lewinsohn, and E.P. Simonen
$20.00