00652 PITTING CORROSION IN DOMESTIC COPPER PLUMBING THE RISE AND FALL OF THE "PITTING WATER" THEORY

Product Number: 51300-00652-SG
ISBN: 00652 2000 CP
Author: Peter F. Ellis II
$0.00
$20.00
$20.00
The theory that "pitting water"--nonaggressive water with high alkalinity and conductivity--is the primary cause of pitting of cold water copper domestic piping appeared in the literature in 1971. This theory gained popularity for a period of time. However, the accumulation of further evidence showed that the theory was non-predictive, and its original proponents retracted it in the 1980' s. Nonetheless, "pitting water" is blamed for pitting of copper domestic plumbing with disturbing frequency more than a decade after the original proponents of the theory withdrew it. A critical review of the literature is presented showing how the "pitting water" theory arose and tracing the accumulation of evidence that invalidates this theory. The case is presented that the concept of "pitting water" is not mechanistically significant, and that most, if not, all pitting of domestic copper plumbing attributed to "pitting water," is in fact of anthropogenic (human-caused) origin.
The theory that "pitting water"--nonaggressive water with high alkalinity and conductivity--is the primary cause of pitting of cold water copper domestic piping appeared in the literature in 1971. This theory gained popularity for a period of time. However, the accumulation of further evidence showed that the theory was non-predictive, and its original proponents retracted it in the 1980' s. Nonetheless, "pitting water" is blamed for pitting of copper domestic plumbing with disturbing frequency more than a decade after the original proponents of the theory withdrew it. A critical review of the literature is presented showing how the "pitting water" theory arose and tracing the accumulation of evidence that invalidates this theory. The case is presented that the concept of "pitting water" is not mechanistically significant, and that most, if not, all pitting of domestic copper plumbing attributed to "pitting water," is in fact of anthropogenic (human-caused) origin.
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for 98709 CORROSION FAILURES OF COPPER/COPPER
Available for download

98709 CORROSION FAILURES OF COPPER/COPPER ALLOY PIPING IN BUILDING PIPING SYSTEMS

Product Number: 51300-98709-SG
ISBN: 98709 1998 CP
Author: Richard A. Hoffmann
$20.00
Picture for 01486 FAILURES OF COPPER POTABLE WATER PIPING
Available for download

01486 FAILURES OF COPPER POTABLE WATER PIPING DUE TO DESIGN, MATERIALS AND POOR WORKMANSHIP

Product Number: 51300-01486-SG
ISBN: 01486 2001 CP
Author: R.S. Charlton
$20.00
Picture for 96294 THE INFLUENCE OF POTABLE WATER
Available for download

96294 THE INFLUENCE OF POTABLE WATER BIOFILMS ON COPPER CORROSION

Product Number: 51300-96294-SG
ISBN: 96294 1996 CP
Author: BJ Webster, DB Wells, PJ Bremer