00235 LASER CLADDING OF NICKEL AND IRON BASE ALLOYS ON BOILER WATERWALL PANELS AND TUBES

Product Number: 51300-00235-SG
ISBN: 00235 2000 CP
Author: Michael S. Brennan and Dr. Roland C. Gassmann
Industry: Energy Generation
$0.00
$20.00
$20.00
Three industries (power generation, paper and steel) have been faced with finding means to protect and extend the operating cycles of their boilers due either to the fuel they burn, method of combustion, and/or the impact of environmental regulations. A common method to protect these tube surfaces is to use weld overlays. In coal-fired boilers with tangential or wall mounted Low NOx burners, corrosion resistant overlays are being used to lower wastage rates caused by the reduced environment above the burners. Also, in some cases high ash levels have resulted in the need for erosion resistant overlays around soot blower openings and sloped walls. Cyclone, fluidized-bed, and basic oxygen furnace (BOF) boilers use ovedays to resist particle erosion. Black liquor recovery boilers and waste-to-energy boilers use overlays to resist corrosion damage from the fuels being burned. As an improved overlay alternative, the laser cladding process: (1) produces a very low dilution overlay (typically 5%) to obtain the optimum benefits of the alloy being deposited even at a low thickness of 0.020" (0.5mm) and (2) increases the selection range of materials since the process can utilize powders [1].
Three industries (power generation, paper and steel) have been faced with finding means to protect and extend the operating cycles of their boilers due either to the fuel they burn, method of combustion, and/or the impact of environmental regulations. A common method to protect these tube surfaces is to use weld overlays. In coal-fired boilers with tangential or wall mounted Low NOx burners, corrosion resistant overlays are being used to lower wastage rates caused by the reduced environment above the burners. Also, in some cases high ash levels have resulted in the need for erosion resistant overlays around soot blower openings and sloped walls. Cyclone, fluidized-bed, and basic oxygen furnace (BOF) boilers use ovedays to resist particle erosion. Black liquor recovery boilers and waste-to-energy boilers use overlays to resist corrosion damage from the fuels being burned. As an improved overlay alternative, the laser cladding process: (1) produces a very low dilution overlay (typically 5%) to obtain the optimum benefits of the alloy being deposited even at a low thickness of 0.020" (0.5mm) and (2) increases the selection range of materials since the process can utilize powders [1].
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for 00247 Erosion-Corrosion Behavior Under Fluidized
Available for download

00247 Erosion-Corrosion Behavior Under Fluidized-Bed Waste Incinerator Conditions

Product Number: 51300-00247-SG
ISBN: 00247 2000 CP
Author: Manabu Noguchi, Hiroshi Yakuwa and Matsuho Miyasaka, Hideyuki Sakamoto and Shigeru Kosugi
$20.00
Picture for 00222 STRESS CORROSION CRACK GROWTH IN ALLOY
Available for download

00222 STRESS CORROSION CRACK GROWTH IN ALLOY 600 EXPOSED TO PWR AND BWR ENVIRONMENTS

Product Number: 51300-00222-SG
ISBN: 00222 2000 CP
Author: Markus O. Speidel and Ruth Magdowski
$20.00
Picture for 00258 Corrosion & Erosion/Corrosion Protection
Available for download

00258 Corrosion & Erosion/Corrosion Protection by Modern Weld Overlays in Low NOx, Coal-Fired Boilers

Product Number: 51300-00258-SG
ISBN: 00258 2000 CP
Author: George Lai and Philip Hulsizer
$20.00