This paper describes the sulfide stress corrosion (SCC) resistance of weldments in 410 stainless steel and 17-4PH precipitation hardening stainless steel. 410 stainless steel weldments with a post weld stress relief heat treatment had a severe reduction in sulfide stress corrosion resistance when compared to the base metal. Austenitizing after welding significantly improves the sulfide stress corrosion resistance of the weldments. 410 stainless steel weldments and base metal with a 900°C (1650°F) austenitizing temperature have a higher resistance to sulfide stress corrosion cracking than with a 982°C (1800°F) austenitizing treatment. The 17-4PH results comparing solution annealing versus aging alone after welding were less conclusive, but weldment sulfide stress corrosion resistance equal to the base metal could be achieved with proper post weld heat treatment. Keywords: sulfide stress cracking, SSC, stainless steel, martensitic, precipitation hardening, pH, chlorides
This paper describes the sulfide stress corrosion (SCC) resistance of weldments in 410 stainless steel and 17-4PH precipitation hardening stainless steel. 410 stainless steel weldments with a post weld stress relief heat treatment had a severe reduction in sulfide stress corrosion resistance when compared to the base metal. Austenitizing after welding significantly improves the sulfide stress corrosion resistance of the weldments. 410 stainless steel weldments and base metal with a 900°C (1650°F) austenitizing temperature have a higher resistance to sulfide stress corrosion cracking than with a 982°C (1800°F) austenitizing treatment. The 17-4PH results comparing solution annealing versus aging alone after welding were less conclusive, but weldment sulfide stress corrosion resistance equal to the base metal could be achieved with proper post weld heat treatment. Keywords: sulfide stress cracking, SSC, stainless steel, martensitic, precipitation hardening, pH, chlorides
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for 00152 CORROSION PERFORMANCE OF 13CR STAINLESS
Available for download

00152 CORROSION PERFORMANCE OF 13CR STAINLESS STEELS

Product Number: 51300-00152-SG
ISBN: 00152 2000 CP
Author: Trond Rogne, John M. Drugli, Ole Oystein Knudsen, Stein Olsen and Jakob Enerhaug
$20.00
Picture for 00156 MATERIALS OPTIMISATION FOR OIL AND
Available for download

00156 MATERIALS OPTIMISATION FOR OIL AND GAS SOUR PRODUCTION

Product Number: 51300-00156-SG
ISBN: 00156 2000 CP
Author: Bijan Kermani
$20.00
Picture for 00157 LIMITS OF LINEPIPE WELD HARDNESS FOR
Available for download

00157 LIMITS OF LINEPIPE WELD HARDNESS FOR DOMAINS OF SOUR SERVICE IN OIL AND GAS PRODUCTION

Product Number: 51300-00157-SG
ISBN: 00157 2000 CP
Author: M B Kermani, C Boucher, J L Crolet, J Enerhaug, P Fassina, R Howard, J p Jansen, C Linne, R Popperli
$20.00