51314-4028-Role of the Grain Orientation Spread in the Pitting Corrosion Resistance of Duplex Stainless Steels

Product Number: 51314-4028-SG
ISBN: 4028 2014 CP
Author: Sandra Le Manchet
Publication Date: 2014
$0.00
$20.00
$20.00
Duplex stainless steels (DSS) are highly important engineering materials due to their generally high corrosion resistance combined with high strength and moderate alloy cost (lower nickel and molybdenum content) compared to standard austenitic grades. They are widely used in various industrial sectors such as oil & gas (pipelines and storage tanks) desalination (evaporators and pumps) and pulp and paper (digester and bleaching reactors) industries. In this paper the influence of the grain orientation spread (GOS) on the corrosion resistance of DSS was investigated in sodium chloride solution.Corrosion measurements were carried out at the microscale by combining the critical pitting temperature (CPT) method the electrochemical microcell technique and a Peltier heating microstage (temperature range from -20 to 120°C). Sites were previously selected according to their GOS value. This value was calculated from the crystallographic orientation map derived from electron backscatter diffraction (EBSD) measurements. The GOS gives a quantitative description of the crystallographic orientation gradients in individual grains.CPT measurements were carried out in various sites at the specimen surface: in austenite grains in ferrite grains at the austenite/ferrite interface with a ratio of 50/50 and in austenite grains containing extremely small ferrite grains. It has been shown that extremely small ferrite grains with a GOS value greater than 1.3° were systematically precursor sites for pitting. The CPT range was 45–90 °C. It was also found that other grains remained passive up to 100 °C.
Duplex stainless steels (DSS) are highly important engineering materials due to their generally high corrosion resistance combined with high strength and moderate alloy cost (lower nickel and molybdenum content) compared to standard austenitic grades. They are widely used in various industrial sectors such as oil & gas (pipelines and storage tanks) desalination (evaporators and pumps) and pulp and paper (digester and bleaching reactors) industries. In this paper the influence of the grain orientation spread (GOS) on the corrosion resistance of DSS was investigated in sodium chloride solution.Corrosion measurements were carried out at the microscale by combining the critical pitting temperature (CPT) method the electrochemical microcell technique and a Peltier heating microstage (temperature range from -20 to 120°C). Sites were previously selected according to their GOS value. This value was calculated from the crystallographic orientation map derived from electron backscatter diffraction (EBSD) measurements. The GOS gives a quantitative description of the crystallographic orientation gradients in individual grains.CPT measurements were carried out in various sites at the specimen surface: in austenite grains in ferrite grains at the austenite/ferrite interface with a ratio of 50/50 and in austenite grains containing extremely small ferrite grains. It has been shown that extremely small ferrite grains with a GOS value greater than 1.3° were systematically precursor sites for pitting. The CPT range was 45–90 °C. It was also found that other grains remained passive up to 100 °C.
Product tags
Also Purchased
Picture for Stress Corrosion Cracking Resistance of Candidate A-USC Alloys
Available for download

51314-3981-Stress Corrosion Cracking Resistance of Candidate A-USC Alloys

Product Number: 51314-3981-SG
ISBN: 3981 2014 CP
Author: James Crum
Publication Date: 2014
$20.00
Picture for Corrosion behavior of Cr bearing low alloy steel with different Cr content in CO2 Top-of-Line Corros
Available for download

51314-4014-Corrosion behavior of Cr bearing low alloy steel with different Cr content in CO2 Top-of-Line Corrosion environment

Product Number: 51314-4014-SG
ISBN: 4014 2014 CP
Author: Yunan Zhang
Publication Date: 2014
$20.00
Picture for Corrosion Behavior of Carbon Steel under Regenerator Conditions in a MDEA-Based CO2 Capture Plant
Available for download

51314-4010-Corrosion Behavior of Carbon Steel under Regenerator Conditions in a MDEA-Based CO2 Capture Plant

Product Number: 51314-4010-SG
ISBN: 4010 2014 CP
Author: Yong Xiang
Publication Date: 2014
$20.00