1391 total products found.
Picture for 03699 AC Interference - Important Issues
Available for download

03699 AC Interference - Important Issues for Cross Country Pipelines

Product Number: 51300-03699-SG
ISBN: 03699 2003 CP
Author: Douglas E. Gilroy
$20.00
Picture for Test Devices to Assess SCC in Ultra High Pressure of H2S
Available for download

51313-02524-Test Devices to Assess SCC in Ultra High Pressure of H2S

Product Number: 51313-02524-SG
ISBN: 02524 2013 CP
Author: Giovanna Gabetta
Publication Date: 2013
$20.00
Picture for CP of Offshore Jacket by Remote Anode Sleds and Discussion About Current Drain to Buried Structures
Available for download

51313-02121-CP of Offshore Jacket by Remote Anode Sleds and Discussion About Current Drain to Buried Structures

Product Number: 51313-02121-SG
ISBN: 02121 2013 CP
Author: Svenn Magne Wigen
Publication Date: 2013
$20.00
Picture for Low Temperature Effect on Sulfide Stress Crack Initiation in Low Alloy Steels
Available for download

Low Temperature Effect on Sulfide Stress Crack Initiation in Low Alloy Steels

Product Number: 51319-12856-SG
Author: Brian Chambers
Publication Date: 2019
$20.00

Exposure temperature has a known effect on sulfide stress cracking (SSC) where elevated temperatures permit the use of oil country tubular goods (OCTG) in sour conditions that would not be survivable at lower temperatures. In order to assess SSC susceptibility NACE MR0175 / ISO15156-2 and API 5CT advise or require the use of room temperature NACE exposure tests in H2S-containing brines and consequently the bulk of qualification data on OCTG has been obtained at these conditions. Previous publications have demonstrated the effect of lower temperatures e.g. 40°F testing on KISSC values of low alloy steel using double cantilever beam (DCB) tests showing a reduction on sour toughness when the temperature is lowered from 75°F to 40°F. This KISSC data provides a clear indication of SSC severity at 40°F on crack propagation; however very little data is available pertinent to crack initiation at temperatures lower than 75°F.In this work several crack initiation tests were performed in mild sour conditions and demonstrated that at low temperature crack initiation susceptibility is increased. Details of the results are discussed within the context of traditional SSC qualification tests and materials selection standards along with the theoretical understanding of SSC fundamentals. Cracking tendency and time-to-failure are reviewed within the context of environmental and material parameters that are altered by the exposure temperature including hydrogen diffusion corrosion rate dissolved H2S concentration and the behavior of hydrogen traps.

Picture for Understanding Alkalinity for Use in Corrosion Prediction
Available for download

Understanding Alkalinity for Use in Corrosion Prediction

Product Number: 51324-21064-SG
Author: Bruce Brown; Yougui Zheng; Jason Dreher; Marc Singer
Publication Date: 2024
$40.00
Picture for 99608 The Full Ring Test Enables Detection of
Available for download