09120785 Effect of Ethanol Chemistry on Stress Corrosion Cracking of Carbon Steel in Fuel-Grade Ethanol

Product Number: 32141-09120785-SG
ISBN: 09120785CJ
Author: X. Lou, D. Yang, and P.M. Singh
Publication Date: 2009
$9.75
$13.00
$13.00
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$13.00
$11.05
Product tags
Also Purchased
Picture for 10078 Corrosivity of Anhyddrous Etthanol, Hydrated Ethanol and Fuel E25
Available for download

10078 Corrosivity of Anhyddrous Etthanol, Hydrated Ethanol and Fuel E25 (25% Ethanol/75% Gasoline)

Product Number: 51300-10078-SG
ISBN: 10078 2010 CP
Author: A Moreira, Z Panossian, C Santos, G Bragagnolo, M Gandur and E Monteiro
Publication Date: 2010
$20.00
Picture for 09530 SCC Behavior of Steel in Fuel Ethanol and Butanol
Available for download

09530 SCC Behavior of Steel in Fuel Ethanol and Butanol

Product Number: 51300-09530-SG
ISBN: 09530 2009 CP
Author: Dale McIntyre, Anand Venkatesh, Russell D. Kane
Publication Date: 2009
$20.00
Picture for 09531 Techniques for Monitoring Conditions Leading to SCC of Carbon Steel in Fuel Grade Ethanol
Available for download

09531 Techniques for Monitoring Conditions Leading to SCC of Carbon Steel in Fuel Grade Ethanol

Product Number: 51300-09531-SG
ISBN: 09531 2009 CP
Author: John Beavers, Narasi Sridhar, Feng Gui
Publication Date: 2009
$20.00