08232 Pitting Corrosion Study in an AE44 Magnesium Alloy

Product Number: 51300-08232-SG
ISBN: 08232 2008 CP
Author: Roxanna Alvarez, Augusto Ruiz, and Mark Horstemeyer
Publication Date: 2008
$0.00
$20.00
$20.00
The initiation and growth mechanisms of corrosion pits in an AE44 magnesium alloy, subjected to a wet saline environment, were quantified, and a corrosion mode to explain the phenomena is suggested. Immersion test were carried out in a NaCl 3.5% solution, for different surfaces at room temperature. The corrosion process was evaluated using a laser profilemeter (LP), optical microscopy (OM), scanning electron microscopy (SEM) and energy dispersive X-Ray spectroscopy (EDS). The stereological quantities included the pit density number, pit radius, pit size distribution, and pit coalescence area. A pit corrosion evolution was estimated using the data obtained from the laser Profilemeter.
The initiation and growth mechanisms of corrosion pits in an AE44 magnesium alloy, subjected to a wet saline environment, were quantified, and a corrosion mode to explain the phenomena is suggested. Immersion test were carried out in a NaCl 3.5% solution, for different surfaces at room temperature. The corrosion process was evaluated using a laser profilemeter (LP), optical microscopy (OM), scanning electron microscopy (SEM) and energy dispersive X-Ray spectroscopy (EDS). The stereological quantities included the pit density number, pit radius, pit size distribution, and pit coalescence area. A pit corrosion evolution was estimated using the data obtained from the laser Profilemeter.
Product tags
Also Purchased
Picture for 08213 Design of Novel Corrosion Inhibiting Additives
Available for download

08213 Design of Novel Corrosion Inhibiting Additives

Product Number: 51300-08213-SG
ISBN: 08213 2008 CP
Author: Jeannine Elliott and Ronald Cook
Publication Date: 2008
$20.00
Picture for 08227 Internal Inspection of 32" Red Hill Pipeline
Available for download

08227 Internal Inspection of 32" Red Hill Pipeline

Product Number: 51300-08227-SG
ISBN: 08227 2008 CP
Author: Terri Regin, Mike Denham, and Marco Campos
Publication Date: 2008
$20.00
Picture for 08230 A Pure Ternary High Molybedenum Containing Ni-Cr-Mo Alloy N06059 (Alloy 59), Provides Reliable
Available for download