07RTS4 Predicting the Effect of Applied Potential on Crack Tip Hydrogen Concentration in Low Alloy Martensitic Steels

Product Number: 51300-07RTS4-SG
ISBN: 07RTS4 2007 CP
Author: Beth Anne Kehler and John R. Scully
Publication Date: 2007
$0.00
$20.00
$20.00
We characterize the dependency of hydrogen embrittlement crack initiation on potential of an ultra high strength steel. This is accomplished through (1) prediction of crack tip hydrogen concentration (CH,tip) as a function of material, geometry, and chemistry of the bulk environment, (2) definition of subsequent crack chemistry and potential, (3) development of a database of diffusible hydrogen concentration (CH,diff) as a function of local chemistry and potential, and (4) use of damage models that predict the threshold stress intensity for cracking (KTH) as a function of CH,tip. In this paper the primary material selected for study is UNS K92580 (AerMet 100), which is characterized by high purity (i.e., low sulfur and phosphorus content) and nano-scale strengthening solute zones and coherent precipitates. The experimental relationship between applied potential and the threshold stress intensity for cracking (KTH) has been established previously for UNS K92580 through slow strain rate testing in an aqueous environment over a range of cathodic and anodic applied potentials. 1 The results reveal a window of applied potentials where there is reduced susceptibility to hydrogen environment embrittlement (HEE). Damage models for initiation and growth can justify this behavior based on the potential dependent value of CH,tip. However, the applied potential itself does not yield insight as to the exact conditions at the crack tip. Ohmic potential (IR) drop and electrochemical/chemical reactions in the crack can lead to a significantly different environment at the crack tip than on the bulk surface. Potential-pH conditions in the crack environment are defined as a function of material, geometry, and chemistry, and then connected to CH,tip, which can then serve as inputs to damage models for HEE initiation and growth.
We characterize the dependency of hydrogen embrittlement crack initiation on potential of an ultra high strength steel. This is accomplished through (1) prediction of crack tip hydrogen concentration (CH,tip) as a function of material, geometry, and chemistry of the bulk environment, (2) definition of subsequent crack chemistry and potential, (3) development of a database of diffusible hydrogen concentration (CH,diff) as a function of local chemistry and potential, and (4) use of damage models that predict the threshold stress intensity for cracking (KTH) as a function of CH,tip. In this paper the primary material selected for study is UNS K92580 (AerMet 100), which is characterized by high purity (i.e., low sulfur and phosphorus content) and nano-scale strengthening solute zones and coherent precipitates. The experimental relationship between applied potential and the threshold stress intensity for cracking (KTH) has been established previously for UNS K92580 through slow strain rate testing in an aqueous environment over a range of cathodic and anodic applied potentials. 1 The results reveal a window of applied potentials where there is reduced susceptibility to hydrogen environment embrittlement (HEE). Damage models for initiation and growth can justify this behavior based on the potential dependent value of CH,tip. However, the applied potential itself does not yield insight as to the exact conditions at the crack tip. Ohmic potential (IR) drop and electrochemical/chemical reactions in the crack can lead to a significantly different environment at the crack tip than on the bulk surface. Potential-pH conditions in the crack environment are defined as a function of material, geometry, and chemistry, and then connected to CH,tip, which can then serve as inputs to damage models for HEE initiation and growth.
Product tags
Also Purchased
Picture for 07697 DEVELOPMENT OF INTERNAL ANTI-CORROSION COATING TECHNOLOGY FOR SOUR GAS GATHERING PIPELINES
Available for download

07697 DEVELOPMENT OF INTERNAL ANTI-CORROSION COATING TECHNOLOGY FOR SOUR GAS GATHERING PIPELINES

Product Number: 51300-07697-SG
ISBN: 07697 2007 CP
Author: Qibin Zhang*, Liping Zhang, Yanjun Zhang, Cuizhu Xu, and Beibei Xie
Publication Date: 2007
$20.00
Picture for 07RTS9 Novel Techniques to Mitigate Corrosion and Stress Corrosion Cracking in Supercritical Water
Available for download

07RTS9 Novel Techniques to Mitigate Corrosion and Stress Corrosion Cracking in Supercritical Water

Product Number: 51300-07RTS9-SG
ISBN: 07RTS9 2007 CP
Author: Todd R. Allen and Gary S. Was
Publication Date: 2007
$20.00
Picture for 07698 The Influence of Microstructure in the Fabrication and Electropolish Finish of Corrosion Resis
Available for download

07698 The Influence of Microstructure in the Fabrication and Electropolish Finish of Corrosion Resistant Equipment for the Bio-Pharmaceutical Industry

Product Number: 51300-07698-SG
ISBN: 07698 2007 CP
Author: Brian Uhlenkamp and Hira S. Ahluwalia
Publication Date: 2007
$20.00