06213 PITTING CORROSION OF STAINLESS STEELS CAUSED BY DISSOLVING SODIUM CHLORIDE UNDER HEAT TRANSFER CONDITIONS

Product Number: 51300-06213-SG
ISBN: 06213 2006 CP
Author: Thomas L. Ladwein
$0.00
$20.00
$20.00
Initiation of local corrosion of stainless steels UNS S 30400 and UNS S 31603 by dissolving sodium chloride under heat transfer conditions has been studied by means of ferroxyl-test and electrochemical noise measurements. Both methods clearly show, that under the conditions of dissolving salt at high wall temperature local corrosion is initiated whereas the conditions of the bulk solution are not critical yet.

Key words: UNS S 30400, UNS S 31603, pitting corrosion, heat transfer, dissolving sodium chloride
Initiation of local corrosion of stainless steels UNS S 30400 and UNS S 31603 by dissolving sodium chloride under heat transfer conditions has been studied by means of ferroxyl-test and electrochemical noise measurements. Both methods clearly show, that under the conditions of dissolving salt at high wall temperature local corrosion is initiated whereas the conditions of the bulk solution are not critical yet.

Key words: UNS S 30400, UNS S 31603, pitting corrosion, heat transfer, dissolving sodium chloride
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for 11255 Pitting Corrosion Mechanisms of Lean Duplex
Available for download

11255 Pitting Corrosion Mechanisms of Lean Duplex, Duplex and Super Duplex Stainless Steels in Chloride Solutions

Product Number: 51300-11255-SG
ISBN: 2011 11255 CP
Author: J. Saithala, J. Atkinson, H Ubhi, A. Patil
Publication Date: 2011
$20.00
Picture for 01414 ADVANCES IN MATERIALS FOR SODIUM
Available for download

01414 ADVANCES IN MATERIALS FOR SODIUM HYPOCHLORITE SERVICE

Product Number: 51300-01414-SG
ISBN: 01414 2001 CCP
Author: Steve Drake
$20.00
Picture for 04303 Electrochemical Evaluation of Stainless
Available for download

04303 Electrochemical Evaluation of Stainless Steels in Acidic Sodium Chloride Solutions

Product Number: 51300-04303-SG
ISBN: 04303 2004 CP
Author: Luz Marina Calle and Louis G. MacDowell, NASA Kennedy Space Center; Rubiela Vinje, ASRC Aerospace
$20.00